MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Overview of materials for Silicone Polyurethane, Ether Based
Categories: Polymer; Thermoplastic; Polyurethane, TP; Silicone Polyurethane, Ether Based

Material Notes: This property data is a summary of similar materials in the MatWeb database for the category "Silicone Polyurethane, Ether Based". Each property range of values reported is minimum and maximum values of appropriate MatWeb entries. The comments report the average value, and number of data points used to calculate the average. The values are not necessarily typical of any specific grade, especially less common values and those that can be most affected by additives or processing methods.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.978 - 1.11 g/cc0.0353 - 0.0401 lb/in³Average value: 1.05 g/cc Grade Count:9
Molecular Weight 95000 g/mol95000 g/molAverage value: 95000 g/mol Grade Count:4
Linear Mold Shrinkage 0.0110 - 0.0360 cm/cm0.0110 - 0.0360 in/inAverage value: 0.0204 cm/cm Grade Count:5
Linear Mold Shrinkage, Transverse 0.00800 - 0.0230 cm/cm0.00800 - 0.0230 in/inAverage value: 0.0148 cm/cm Grade Count:3
Melt Flow 2.00 - 37.0 g/10 min2.00 - 37.0 g/10 minAverage value: 21.2 g/10 min Grade Count:5
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 55.0 - 95.055.0 - 95.0Average value: 76.1 Grade Count:15
Hardness, Shore D 50.0 - 80.050.0 - 80.0Average value: 65.1 Grade Count:7
Tensile Strength, Ultimate 12.0 - 60.0 MPa1740 - 8700 psiAverage value: 29.8 MPa Grade Count:22
Elongation at Break 25.0 - 823 %25.0 - 823 %Average value: 453 % Grade Count:22
Modulus of Elasticity 0.00800 - 0.750 GPa1.16 - 109 ksiAverage value: 0.188 GPa Grade Count:12
Flexural Yield Strength 1.45 - 1.86 MPa210 - 270 psiAverage value: 1.61 MPa Grade Count:3
Flexural Modulus 0.0371 - 0.0433 GPa5.38 - 6.28 ksiAverage value: 0.0396 GPa Grade Count:3
Tear Strength 20.2 - 175 kN/m115 - 999 pliAverage value: 72.6 kN/m Grade Count:19
Taber Abrasion, mg/1000 Cycles 5.40 - 85.05.40 - 85.0Average value: 29.7 Grade Count:5
Compression Set 15.0 - 29.0 %15.0 - 29.0 %Average value: 21.7 % Grade Count:9
 
Electrical PropertiesMetricEnglishComments
Dielectric Constant 5.70 - 7.005.70 - 7.00Average value: 6.28 Grade Count:5
Dielectric Strength 11.8 - 16.5 kV/mm300 - 420 kV/inAverage value: 13.7 kV/mm Grade Count:5
 
Thermal PropertiesMetricEnglishComments
CTE, linear 187 - 200 µm/m-°C104 - 111 µin/in-°FAverage value: 192 µm/m-°C Grade Count:5
Vicat Softening Point 67.0 - 82.0 °C153 - 180 °FAverage value: 74.0 °C Grade Count:3
Glass Transition Temp, Tg -68.0 - -12.0 °C-90.4 - 10.4 °FAverage value: -35.7 °C Grade Count:3
 
Processing PropertiesMetricEnglishComments
Processing Temperature 182 - 204 °C360 - 399 °FAverage value: 193 °C Grade Count:5
Drying Temperature 82.0 - 104 °C180 - 219 °FAverage value: 93.0 °C Grade Count:3
Moisture Content 0.0100 %0.0100 %Average value: 0.0100 % Grade Count:4

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Overview of materials for Thermoplastic Polyurethane, Elastomer, Ether Grade
Overview of materials for Thermoplastic Polyurethane (TPUR), Glass Fiber Reinforced
Overview of materials for Thermoplastic Polyurethane, Elastomer, Polyester Grade
Overview of materials for Silicone Polyurethane, Polycarbonate Based
Overview of materials for Silicone Rubber

O5050 / 78467

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.