MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

American White Spruce Wood
Categories: Wood and Natural Products; Wood; Softwood

Material Notes: Large sizes available. Conifer
Usual surface texture: Medium
Dimensional changes when dried lumber is subjected to variations in humidity during service: Small
Resistance to fungal decay (Heartwood in ground contact): Non-durable (5 to 10 years)
Resistance to penetration by preservatives: Resistant
Common Applications: Construction, joinery

Property values marked by an asterisk (*) have been taken from an unusually old reference source.

Key Words: Picea glauca; Lumber, Timber
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.370 g/cc0.0134 lb/in³Oven Dry Weight/Unseasoned Volume
 0.561 g/cc0.0203 lb/in³Unseasoned*
 
Mechanical PropertiesMetricEnglishComments
Hardness, Wood Indentation 1200 N270 lb (f)Side. Force required to imbed a 0.444 inch steel ball to one-half its diameter
 1300 N292 lb (f)End. Force required to imbed a 0.444 inch steel ball to one-half its diameter
Tensile Strength, Ultimate 1.38 MPa200 psiPerpendicular to Grain*
Modulus of Rupture 0.0372 GPa5.40 ksiStatic Bending*
Flexural Yield Strength 22.8 MPa3300 psiFiber Stress at Elastic Limit; Static Bending*
Flexural Modulus 6.76 GPa980 ksiStatic Bending*
Compressive Strength 1.86 MPa270 psiPerpendicular to Grain*
 15.7 MPa2280 psiParallel to Grain*
 16.4 MPa2380 psiMax Crushing Strength Parallel to Grain*
Machinability 100 %100 %Good Relative to Other Wood
Shear Strength 4.62 MPa670 psiParallel to Grain*
Impact 2.02.0in-lb/in³; Work to Elastic Limit; Unseasoned Sample; Impact Bending*
 68006800psi; Fiber Stress at Elastic Limit; Unseasoned Sample; Impact Bending*
Work to Elastic Limit 0.00455 J/cm³0.660 in-lb/in³Static Bending*
Work to Maximum Load 0.0393 J/cm³5.70 in-lb/in³Static Bending*
 
Thermal PropertiesMetricEnglishComments
Thermal Conductivity 0.0908 W/m-K0.630 BTU-in/hr-ft²-°FOven Dry
 0.108 W/m-K0.750 BTU-in/hr-ft²-°F12% Moisture Content
Shrinkage 4.7 %4.7 %Radial; Unseasoned to Oven Dry*
 8.2 %8.2 %Tangential; Unseasoned to Oven Dry*
 13.4 %13.4 %Volumetric; Unseasoned to Oven Dry*
 
Descriptive Properties
ColorWhite to pale yellow-brownUsual for heartwood

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
American Red Spruce Wood
Canadian Spruce Wood
American Balsam Fir Wood
American Red Western Cedar (Giant Arborvitae) Wood
American Rocky Mountain Douglas Fir Wood

PTSA590 / 71266

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.