System Message
Advertise with MatWeb!
Data sheets for over
180,000
metals, plastics, ceramics, and composites.
HOME
•
SEARCH
•
TOOLS
•
SUPPLIERS
•
FOLDERS
•
ABOUT US
•
FAQ
•
LOG IN
Recently Viewed Materials (most recent at top)
Login
to see your most recently viewed materials here.
Or if you don't have an account with us yet, then
click here to register.
Searches:
Advanced
|
Category
|
Property
|
Metals
|
Trade Name
|
Manufacturer
|
Recently Viewed Materials
Encom Polymers EnLon PX7006 Amorphous Nylon, 30% Glass Filled
Categories:
Polymer
;
Thermoplastic
;
Nylon (Polyamide PA)
;
Amorphous Nylon
Material Notes:
Appearance: Black
Processing Methods: Injection Molding
Applications: Suitable for use as Metal Replacement
Information provided by EnCom Polymers
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Metric
English
Comments
Specific Gravity
1.22
g/cc
1.22
g/cc
ASTM D792
Filler Content
30 %
30 %
Water Absorption
3.1 %
3.1 %
65% RH Equilibrium; ASTM D570
5.8 %
5.8 %
Water Immersion Equilibrium; ASTM D570
Maximum Moisture Content
0.020
0.020
Linear Mold Shrinkage, Flow
0.00
cm/cm
@Thickness 3.20 mm
0.00
in/in
@Thickness 0.126 in
ASTM D955
Melt Flow
40
g/10 min
@Load 2.16 kg,
Temperature 275 °C
40
g/10 min
@Load 4.76 lb,
Temperature 527 °F
ASTM D1238
Mechanical Properties
Metric
English
Comments
Tensile Strength, Yield
100
MPa
14500
psi
ASTM D638
Elongation at Break
2.3 %
2.3 %
ASTM D638
Tensile Modulus
4.828
GPa
700.2
ksi
ASTM D638
Flexural Strength
166
MPa
24100
psi
ASTM D790
Flexural Modulus
4.483
GPa
650.2
ksi
ASTM D790
Izod Impact, Notched
0.430
J/cm
0.806
ft-lb/in
ASTM D256
Thermal Properties
Metric
English
Comments
Deflection Temperature at 0.46 MPa (66 psi)
96.0
°C
205
°F
ASTM D648
Flammability, UL94
HB
@Thickness 1.60 mm
HB
@Thickness 0.0630 in
Processing Properties
Metric
English
Comments
Rear Barrel Temperature
260
-
282
°C
500
-
540
°F
Middle Barrel Temperature
266
-
288
°C
510
-
550
°F
Front Barrel Temperature
271
-
293
°C
520
-
560
°F
Nozzle Temperature
271
-
293
°C
520
-
560
°F
Melt Temperature
271
-
293
°C
520
-
560
°F
Drying Temperature
79.4
°C
175
°F
Dry Time
2.00
-
12.0
hour
2.00
-
12.0
hour
Back Pressure
0.172
-
0.517
MPa
25.0
-
75.0
psi
Shot Size
25 - 75 %
25 - 75 %
Vent Depth
0.00254
cm
0.00100
in
Screw Speed
60
-
120
rpm
60
-
120
rpm
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to view all the property values for this datasheet as they were originally entered into MatWeb.
PENCOM020 / 266034
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
webmaster@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.