MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Total 7231X Polypropylene, Blow Molding Grade  (discontinued **)
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene, Blow Molding Grade

Material Notes: Random copolymer blow molding grade with improved impact and clarity

Impact Strength -- FINA 7231X offers excellent impact strength, clarity and gloss.

Lubricated -- FINA 7231X offers superior core rod release for ease in processing.

High Purity - FINA 7231X features minimum taste and odor, and optimum thermal stability for superior color and processability.

FDA -- FINA 7231X complies with all applicable FDA regulations and may be used under these provisions for food contact and packaging.

Recommended Applications -- FINA 7231X is recommended for blow molded containers for food, drug, cosmetic and toiletry applications requiring superior impact strength and clarity.

Processing -- FINA 7231X resin processes on conventional blow molding equipment with typical melt temperatures of 390-450°F (177- 232°C)

Data provided by the manufacturer, Total Petrochemicals.

Total Petrochemicals includes former Fina and Atofina plastics product lines.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Water Vapor Permeability 9.40 g mil/ (m2 day)
@Temperature 37.8 °C
0.606 g mil/ (100 in2 day)
@Temperature 100 °F
90% RH; ASTM E96
Density 0.900 g/cc0.0325 lb/in³ASTM D1505
Oxygen Transmission 95.0 cc-mm/m²-24hr-atm
@Temperature 23.0 °C
241 cc-mil/100 in²-24hr-atm
@Temperature 73.4 °F
cc-mm/m²-24hr-atm; ASTM D1434
Melt Flow 2.0 g/10 min2.0 g/10 minASTM D1238L
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Ultimate 23.4 MPa3390 psiASTM D638
Elongation at Break 11 %11 %ASTM D638
Modulus of Elasticity 0.827 GPa120 ksiASTM D638
Flexural Modulus 0.689 GPa99.9 ksiASTM D790
Izod Impact, Notched 0.694 J/cm1.30 ft-lb/inASTM D256A
 
Thermal PropertiesMetricEnglishComments
Melting Point 143 °C289 °FDSC
Deflection Temperature at 0.46 MPa (66 psi) 88.0 °C190 °FASTM D648
 
Processing PropertiesMetricEnglishComments
Melt Temperature 177 - 232 °C351 - 450 °Fblow molding

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PFIN86 / 38416

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.