MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

CEN® Electronic Material CN Polyimide Film, 6 Mil Thickness
Categories: Polymer; Film; Thermoset; Polyimide, TS; Polyimide, Thermoset Film

Material Notes: CEN®CN polyimide film is typical general-purpose polyimide film and has been used successfully in applications at temperatures as low as -269°C (-452°F) and as high as 400°C (752°F). CN film can be laminated, metallized, punched, formed or adhesive coated. CEN®CN is used for applications that require an all-polyimide film with an excellent balance of properties over a wide range of temperatures.

Applications: mechanical parts, electronic parts, electrical insulation, pressure sensitive tape, fiber optics cable, insulation blankets, insulation tubing, automotive diaphragms sensors and manifolds.

All information provided by CEN Electronic Material Co., LTD.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Thickness 140 - 160 microns5.51 - 6.30 mil
 
Mechanical PropertiesMetricEnglishComments
Film Tensile Strength at Yield, MD 125 MPa18100 psi
Film Tensile Strength at Yield, TD 115 MPa16700 psi
Film Elongation at Yield, MD >= 45 %>= 45 %
Film Elongation at Yield, TD >= 45 %>= 45 %
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity >= 5.00e+12 ohm-cm>= 5.00e+12 ohm-cm
Surface Resistance >= 5.00e+13 ohm>= 5.00e+13 ohm
Dielectric Strength >= 120 kV/mm>= 3050 kV/in

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Caplinq LINQTAPE™ PIT2A
Caplinq LINQTAPE™ PIT1S
Caplinq LINQTAPE™ PIT1A
Caplinq LINQTAPE™ PIT2S
CEN® Electronic Material BL Polyimide Film

PCENE021 / 93483

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.