MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

BCC Products EB 6200 Epoxy Tooling Board
Categories: Polymer; Thermoset; Epoxy; Epoxy Molding Compound

Material Notes: EB6200 is a “grain-free” elevated temperature epoxy modeling material known for its superior surface finish, dimensional stability and the ability to maintain tolerances even after being subjected to temperature variations. EB6200 has excellent dimensional stability results from the low coefficient of thermal expansion and high glass transition temperature. Applications: Master Models (Aerospace); Automotive Die Models; Vacuum Forming at Elevated Temperatures; Lay-Up Tools for Medium and High Temperature Curing Prepreg

Information provided by BCC Products, Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 0.760 g/cc0.760 g/ccASTM-D-792-66
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 7272ASTM D2240
Tensile Strength, Ultimate 30.3 MPa4400 psiASTM D638
Flexural Strength 35.5 MPa5150 psiASTM D790
Flexural Modulus 2.41 GPa349 ksiASTM-D-790
Compressive Strength 33.1 MPa4800 psiASTM D695
Compressive Modulus 2.36 GPa342 ksiASTM-D-695
Izod Impact, Notched 0.299 J/cm0.560 ft-lb/inASTM D256
Izod Impact Unnotched 1.42 J1.05 ft-lbASTM D256
 
Thermal PropertiesMetricEnglishComments
CTE, linear 37.8 µm/m-°C21.0 µin/in-°F
Deflection Temperature at 1.8 MPa (264 psi) 149 °C300 °FASTM-D-648-56
Glass Transition Temp, Tg >= 163 °C>= 325 °FASTM D3418

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
CMT Materials REN Shape® 5008 Vacuum Forming Tooling Board
Solvay CYFORM® 22 Epoxy Tooling Prepreg
Orion Engineered Carbons CORAX® N 234 ASTM Carbon Black
Mitsubishi Chemical Advanced Materials TIVAR® 1000 UHMW-PE, (Natural & Colors except Black) (ASTM Product Data Sheet)
Lord Adhesives Circalok™ EP-729 Epoxy Board Level Encapsulant

PBCC017 / 107244

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.