MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Encom Polymers EnCore F0803U ABS, Flame Retardant, Molding Grade, RoHS Compliant, UV Resistant
Categories: Polymer; Thermoplastic; ABS Polymer; Acrylonitrile Butadiene Styrene (ABS), Unreinforced, Flame Retardant

Material Notes: Appearance: Black, Natural or Colors

Processing Methods: Injection Molding, Profile Extrusion

Applications: Electrical, Electronic Business Equipment

Information provided by EnCom Polymers

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.22 g/cc1.22 g/ccASTM D792
Maximum Moisture Content 0.100.10
Linear Mold Shrinkage, Flow 0.0050 - 0.0080 cm/cm
@Thickness 3.20 mm
0.0050 - 0.0080 in/in
@Thickness 0.126 in
ASTM D955
Linear Mold Shrinkage, Transverse 0.0040 - 0.0070 cm/cm
@Thickness 3.20 mm
0.0040 - 0.0070 in/in
@Thickness 0.126 in
ASTM D955
Melt Flow 8.0 g/10 min
@Load 3.80 kg,
Temperature 230 °C
8.0 g/10 min
@Load 8.38 lb,
Temperature 446 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 38.0 MPa5510 psiASTM D638
Elongation at Break 4.4 %4.4 %ASTM D638
Tensile Modulus 2.207 GPa320.1 ksiASTM D638
Flexural Strength 66.0 MPa9570 psiASTM D790
Flexural Modulus 2.276 GPa330.1 ksiASTM D790
Izod Impact, Notched 1.60 J/cm3.00 ft-lb/inASTM D256
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 1.8 MPa (264 psi) 77.0 °C171 °FASTM D648
Flammability, UL94  V-0
@Thickness 1.57 mm
V-0
@Thickness 0.0620 in
 5VA
@Thickness 3.17 mm
5VA
@Thickness 0.125 in
 
Processing PropertiesMetricEnglishComments
Rear Barrel Temperature 166 - 182 °C330 - 360 °F
Middle Barrel Temperature 177 - 204 °C350 - 400 °F
Front Barrel Temperature 191 - 232 °C375 - 450 °F
Nozzle Temperature 191 - 232 °C375 - 450 °F
Melt Temperature 191 - 232 °C375 - 450 °F
Mold Temperature 48.9 - 76.7 °C120 - 170 °F
Drying Temperature 76.7 - 87.8 °C170 - 190 °F
Dry Time 2.00 - 4.00 hour2.00 - 4.00 hour
 <= 7.00 hour<= 7.00 hour
Back Pressure 0.172 - 0.689 MPa25.0 - 100 psi
Screw Speed 25 - 75 rpm25 - 75 rpm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PENCOM004 / 266018

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.