MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

Plenco 6990 Phenolic, Briquette, Compression Molded  (discontinued **)
Categories: Polymer; Thermoset; Filled/Reinforced Thermoset; Phenolic; Phenolic, Novolac, Mineral/Glass Filled

Material Notes: PLENCO 06990 is a glass and mineral filled novolac phenolic molding compound. UL recognized under component file E40654.

Information supplied by Plenco.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Bulk Density 0.770 g/cc0.0278 lb/in³ASTM D1895
Density 1.78 g/cc0.0643 lb/in³ASTM D792
Water Absorption 0.080 %0.080 %ASTM D570
Linear Mold Shrinkage 0.0017 cm/cm0.0017 in/inASTM D955
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell E 8686ASTM D785
Tensile Strength, Ultimate 51.0 MPa7400 psiASTM D638
Elongation at Break 0.33 %0.33 %ASTM D638
Tensile Modulus 16.8 GPa2440 ksiASTM D638
Flexural Strength 65.0 MPa9430 psiASTM D790
Flexural Modulus 13.5 GPa1960 ksiASTM D790
Compressive Strength 172 MPa24900 psiASTM D695
Izod Impact, Notched 0.410 J/cm0.768 ft-lb/inASTM D256
Charpy Impact, Notched 0.510 J/cm²2.43 ft-lb/in²ASTM D256
Impact 272272J/m Drop Ball Impact; PLENCO
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 8.00e+11 ohm-cm8.00e+11 ohm-cmASTM D247
Dielectric Constant 5.65.6ASTM D150
Dielectric Strength 15.2 kV/mm386 kV/inShort Time; ASTM D149
Dissipation Factor 0.0380.038ASTM D150
Arc Resistance 184 sec184 secASTM D495
Comparative Tracking Index 250 V250 VASTM D3638
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 250 °C482 °FHeat Resistance; ASTM D570D
Deflection Temperature at 1.8 MPa (264 psi) 266 °C511 °FASTM D648
Flammability, UL94 V-0
@Thickness 0.500 mm
V-0
@Thickness 0.0197 in
Shrinkage 0.00060 %0.00060 %72 hr, 120ºC; ASTM D1299

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PLEM21 / 50700

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.