MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Overview of materials for Phenolic, Novolac, Woodflour Filled
Categories: Polymer; Thermoset; Phenolic; Phenolic, Novolac, Woodflour Filled

Material Notes: This property data is a summary of similar materials in the MatWeb database for the category "Phenolic, Novolac, Woodflour Filled". Each property range of values reported is minimum and maximum values of appropriate MatWeb entries. The comments report the average value, and number of data points used to calculate the average. The values are not necessarily typical of any specific grade, especially less common values and those that can be most affected by additives or processing methods.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.36 - 1.43 g/cc0.0491 - 0.0517 lb/in³Average value: 1.40 g/cc Grade Count:31
Water Absorption 0.247 - 0.640 %0.247 - 0.640 %Average value: 0.387 % Grade Count:31
Linear Mold Shrinkage 0.00340 - 0.0109 cm/cm0.00340 - 0.0109 in/inAverage value: 0.00668 cm/cm Grade Count:31
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell E 75.0 - 93.075.0 - 93.0Average value: 86.8 Grade Count:25
Tensile Strength, Ultimate 45.0 - 64.0 MPa6530 - 9280 psiAverage value: 54.5 MPa Grade Count:31
Elongation at Break 0.410 - 0.920 %0.410 - 0.920 %Average value: 0.738 % Grade Count:25
Modulus of Elasticity 7.60 - 9.40 GPa1100 - 1360 ksiAverage value: 8.40 GPa Grade Count:25
Flexural Yield Strength 68.0 - 97.0 MPa9860 - 14100 psiAverage value: 83.4 MPa Grade Count:31
Flexural Modulus 6.80 - 9.00 GPa986 - 1310 ksiAverage value: 7.82 GPa Grade Count:31
Compressive Yield Strength 155 - 234 MPa22500 - 33900 psiAverage value: 208 MPa Grade Count:31
Poissons Ratio 0.330 - 0.3600.330 - 0.360Average value: 0.352 Grade Count:11
Shear Modulus 2.79 - 3.22 GPa405 - 467 ksiAverage value: 3.00 GPa Grade Count:11
Izod Impact, Notched 0.153 - 0.241 J/cm0.287 - 0.451 ft-lb/inAverage value: 0.187 J/cm Grade Count:25
Charpy Impact, Notched 0.178 - 0.249 J/cm²0.847 - 1.19 ft-lb/in²Average value: 0.196 J/cm² Grade Count:25
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 1.60e+11 - 5.00e+13 ohm-cm1.60e+11 - 5.00e+13 ohm-cmAverage value: 2.81e+12 ohm-cm Grade Count:30
Dielectric Constant 4.00 - 6.104.00 - 6.10Average value: 5.09 Grade Count:30
Dielectric Strength 8.50 - 16.7 kV/mm216 - 424 kV/inAverage value: 12.0 kV/mm Grade Count:30
Dissipation Factor 0.0300 - 0.1000.0300 - 0.100Average value: 0.0531 Grade Count:30
Arc Resistance 25.0 - 144 sec25.0 - 144 secAverage value: 119 sec Grade Count:24
Comparative Tracking Index 125 - 200 V125 - 200 VAverage value: 160 V Grade Count:30
 
Thermal PropertiesMetricEnglishComments
CTE, linear 43.0 - 99.0 µm/m-°C
@Temperature 40.0 - 130 °C
23.9 - 55.0 µin/in-°F
@Temperature 104 - 266 °F
Average value: 62.3 µm/m-°C Grade Count:22
Thermal Conductivity 0.340 - 0.440 W/m-K
@Temperature 100 - 100 °C
2.36 - 3.05 BTU-in/hr-ft²-°F
@Temperature 212 - 212 °F
Average value: 0.384 W/m-K Grade Count:15
Maximum Service Temperature, Air 187 - 207 °C369 - 405 °FAverage value: 198 °C Grade Count:25
Deflection Temperature at 1.8 MPa (264 psi) 142 - 186 °C288 - 367 °FAverage value: 168 °C Grade Count:31
UL RTI, Electrical 150 °C302 °FAverage value: 150 °C Grade Count:6
UL RTI, Mechanical with Impact 150 °C302 °FAverage value: 150 °C Grade Count:6
UL RTI, Mechanical without Impact 150 °C302 °FAverage value: 150 °C Grade Count:6
Flammability, UL94 HB - V-1HB - V-1Grade Count:29
Oxygen Index 24.5 - 29.1 %24.5 - 29.1 %Average value: 26.4 % Grade Count:23

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Overview of materials for Phenolic/Glass Fiber SMC
Overview of materials for Phenolic/Rubber; Molded
Overview of materials for Phenolic; Unreinforced; Molded
Bakelite® PF 1110 Phenolic Molding Compound
Overview of materials for Phenolic, Novolac, Impact Grade, Filled

O2710 / 78087

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.