MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

AGC Fluon® LM-720A ETFE
Categories: Polymer; Thermoplastic; Fluoropolymer; ETFE/ECTFE

Material Notes: Description: Fluon® LM-ETFE is a modified ethylene/tetrafluoroethylene (ETFE) polymer. Fluon LM-ETFE is different than most other ETFE materials in that it has a lower melting point (225°C versus 260°C for most ETFE), better chemical resistance and thermal stability, improved optical clarity, better flexibility, and a higher limiting oxygen index (40% versus 31%). It is processable by conventional extrusion and injection molding techniques. Rotomolding and rotolining grades are also available.

Benefits

  • High resistance to heat
  • Excellent chemical resistance
  • Good physical toughness
  • Low smoke and flame characteristics: Fluon LM-ETFE is rated 94 V-0 by Underwriters Laboratories Inc.
  • Outstanding resistance to weather and aging
  • Good dielectric properties
  • Non-stick characteristics
Applications:
  • Film and sheets
  • Valves, fittings, and housings
  • Tubing and pipe
  • Wire & cable
  • Filter media
  • Vessel linings

Information provided by AGC Chemicals Americas Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.78 g/cc1.78 g/ccASTM D792
Melt Flow 25 g/10 min25 g/10 minASTM D3159
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 6565ASTM D2240
Tensile Strength 40.0 MPa5800 psiASTM D638
Elongation at Break 400 %400 %ASTM D638
Flex Crack Resistance 150000150000Cycles per MIT Folding Endurance; ASTM D2176
 
Electrical PropertiesMetricEnglishComments
Dielectric Constant 2.4
@Frequency 1e+6 Hz
2.4
@Frequency 1e+6 Hz
ASTM D150
 
Thermal PropertiesMetricEnglishComments
CTE, linear 124 µm/m-°C
@Temperature 0.000 - 100 °C
69.0 µin/in-°F
@Temperature 32.0 - 212 °F
ASTM D696
Melting Point 225 °C437 °FASTM D3159
Brittleness Temperature -103 °C-153 °FASTM D764
Flammability, UL94 V-0V-0
Oxygen Index 40 %40 %ASTM D2863

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
AGC Fluon® LM-740A ETFE
Avient OnFlex™ S HF 80A-3S1986 Thermoplastic Elastomer (TPE)
AGC Fluon® LM-730AP LM-ETFE Fluororesin
AGC Fluon® LM-730A ETFE
AGC Fluon® LM-720AP LM-ETFE Fluororesin

PAGCX140 / 191249

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.