MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Bangtai 68T90U Polyester Based TPU for T- Die Film
Categories: Polymer; Thermoplastic; Polyurethane, TP; Thermoplastic Polyurethane, Elastomer, Polyester Grade

Material Notes: Processing: Casting film, Calendaring film, T-Die

Properties:: Low melting point, High frequency, Easily cut and suitable for Butt Fusion welding.

Star-level products: 68T85-1 69M95N; Super Transparent, Super low yellowness index, No crystalline grain impurity, Low possibility of small molecule Precipitation

Applications: Shoes, Football covers, Luggage, Adhesive film, Leather, Composite film etc.

Information provided by Baoding Bangtai Polymeric New-materials Co., Ltd

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.20 - 1.24 g/cc0.0434 - 0.0448 lb/in³ASTM D792
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 88 - 9288 - 92ASTM D2240
Tensile Strength 20.0 - 30.0 MPa2900 - 4350 psiASTM D412
Elongation at Break 500 - 800 %500 - 800 %ASTM D412
100% Modulus 11.0 - 15.0 MPa1600 - 2180 psiASTM D412
300% Modulus 9.00 - 15.0 MPa1310 - 2180 psiASTM D412
Tear Strength 78.5 - 137 kN/m448 - 784 pliASTM D624
 
Processing PropertiesMetricEnglishComments
Processing Temperature 190 - 200 °C374 - 392 °F
Drying Temperature 100 - 110 °C212 - 230 °F
Dry Time 1.00 - 2.00 hour1.00 - 2.00 hour
 
Descriptive Properties
UV level=424h, ISO 105-A02:1993/Cor. 2:2005

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PBANGT033 / 312393

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.