MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

SABIC CYCOLAC™ FR15 ABS (Americas)
Categories: Polymer; Thermoplastic; ABS Polymer

Material Notes: Flame retardant ABS (non-PBBE additive). Good property/toughness. Excellent moldability. UL94 V-0/5VA rated.

Information provided by SABIC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.20 g/cc1.20 g/ccASTM D792
Density 1.19 g/cc0.0430 lb/in³ISO 1183
Viscosity 290000 cP
@Shear Rate 1000 1/s,
Temperature 200 °C
290000 cP
@Shear Rate 1000 1/s,
Temperature 392 °F
melt; ASTM D3825
Linear Mold Shrinkage, Flow 0.0050 - 0.0070 cm/cm
@Thickness 3.20 mm
0.0050 - 0.0070 in/in
@Thickness 0.126 in
SABIC method
Melt Flow  4.0 g/10 min
@Load 3.80 kg,
Temperature 230 °C
4.0 g/10 min
@Load 8.38 lb,
Temperature 446 °F
ASTM D1238
 10 g/10 min
@Load 5.00 kg,
Temperature 220 °C
10 g/10 min
@Load 11.0 lb,
Temperature 428 °F
ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 31.0 MPa4500 psi50 mm/min; ISO 527
 35.0 MPa5080 psi5 mm/min; ASTM D638
Tensile Strength, Yield 41.0 MPa5950 psi50 mm/min; ISO 527
 41.0 MPa5950 psi5 mm/min; ASTM D638
Elongation at Break 9.0 %9.0 %5 mm/min; ASTM D638
 33.5 %33.5 %50 mm/min; ISO 527
Elongation at Yield 2.1 %2.1 %50 mm/min; ISO 527
 2.3 %2.3 %5 mm/min; ASTM D638
Tensile Modulus 2.34 GPa339 ksi5 mm/min; ASTM D638
Flexural Yield Strength 71.0 MPa10300 psi1.3 mm/min, 50 mm span; ASTM D790
Flexural Modulus 2.72 GPa395 ksi1.3 mm/min, 50 mm span; ASTM D790
Izod Impact, Notched 2.13 J/cm3.99 ft-lb/inASTM D256
Izod Impact, Notched (ISO) 18.0 kJ/m²8.57 ft-lb/in²80*10*4; ISO 180/1A
 6.00 kJ/m²
@Temperature -30.0 °C
2.86 ft-lb/in²
@Temperature -22.0 °F
80*10*4; ISO 180/1A
Charpy Impact, Notched 1.90 J/cm²9.04 ft-lb/in²Edgew 80*10*4 sp=62mm; ISO 179/1eA
Dart Drop, Total Energy 33.0 J24.3 ft-lbASTM D3763
 
Electrical PropertiesMetricEnglishComments
Arc Resistance 0.00 - 60 sec0.00 - 60 secASTM D495
Comparative Tracking Index 250 - 400 V250 - 400 VUL 746A
Hot Wire Ignition, HWI 15 - 30 sec15 - 30 secUL 746A
High Amp Arc Ignition, HAI 0.00 - 15 arcs0.00 - 15 arcsUL 746A
High Voltage Arc-Tracking Rate, HVTR >= 150 mm/min>= 5.91 in/minUL 746A
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 84.6 µm/m-°C
@Temperature -40.0 - 40.0 °C
47.0 µin/in-°F
@Temperature -40.0 - 104 °F
ASTM E831
CTE, linear, Transverse to Flow 86.4 µm/m-°C
@Temperature -40.0 - 40.0 °C
48.0 µin/in-°F
@Temperature -40.0 - 104 °F
ASTM E831
Deflection Temperature at 0.46 MPa (66 psi) 82.0 °C
@Thickness 3.20 mm
180 °F
@Thickness 0.126 in
unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 73.0 °C163 °FFlatw 80*10*4 sp=64mm; ISO 75/Af
 70.0 °C
@Thickness 3.20 mm
158 °F
@Thickness 0.126 in
unannealed; ASTM D648
Vicat Softening Point 81.0 °C178 °FRate B/50; ISO 306
 84.0 °C183 °FRate B/120; ISO 306
 86.0 °C187 °FRate B/50; ASTM D1525
UL RTI, Electrical 60.0 °C140 °FUL 746B
UL RTI, Mechanical with Impact 60.0 °C140 °FUL 746B
UL RTI, Mechanical without Impact 60.0 °C140 °FUL 746B
Flammability, UL94  V-0
@Thickness 1.49 mm
V-0
@Thickness 0.0587 in
UL 94
 5VA
@Thickness 2.48 mm
5VA
@Thickness 0.0976 in
UL 94
 
Processing PropertiesMetricEnglishComments
Nozzle Temperature 200 - 220 °C392 - 428 °FInjection Molding
Zone 1 170 - 180 °C338 - 356 °F
Zone 2 195 - 205 °C383 - 401 °F
Zone 3 200 - 215 °C392 - 419 °F
Melt Temperature 200 - 220 °C392 - 428 °F
Mold Temperature 50.0 - 70.0 °C122 - 158 °F
Drying Temperature 80.0 - 90.0 °C176 - 194 °FInjection Molding
Dry Time 2.00 - 4.00 hour2.00 - 4.00 hourInjection Molding
 6.00 hour6.00 hourCumulative; Injection Molding
Moisture Content 0.10 %0.10 %
Back Pressure 0.300 - 0.700 MPa43.5 - 102 psi
Shot Size 50 - 70 %50 - 70 %
Vent Depth 0.00380 - 0.00510 cm0.00150 - 0.00201 in
Screw Speed 30 - 60 rpm30 - 60 rpm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PSABI10027 / 243494

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.