MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

AISI Grade 18Ni (350) Maraging Steel, Aged, at RT, tested transverse, sheet 6 mm thick
Categories: Metal; Ferrous Metal; Alloy Steel; Low Alloy Steel; Carbon Steel; Low Carbon Steel; Maraging Steel

Material Notes: Applications: rocket motor cases, load cells, flexures for guidance mechanisms of missiles, helicopter drive shafts, aircraft wing components, aluminum die casting dies, cores, pins, plastic molding dies, trim knees, cold forming dies and springs.

Key Words: UNS K93120
Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 8.08 g/cc0.292 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Ultimate 2451 MPa355500 psi
Tensile Strength, Yield 2395 MPa
@Strain 0.2 %
347400 psi
@Strain 0.2 %
Elongation at Break 3.0 %3.0 %In gage length 4.5 times the square root of the area.
Reduction of Area 15.4 %15.4 %
Modulus of Elasticity 200 GPa29000 ksi
Bulk Modulus 160 GPa23200 ksiTypical for steel.
Poissons Ratio 0.300.30Calculated
Shear Modulus 77.0 GPa11200 ksiEstimated from elastic modulus
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.0000174 ohm-cm0.0000174 ohm-cmTypical steel
 
Thermal PropertiesMetricEnglishComments
CTE, linear 11.3 µm/m-°C
@Temperature 21.0 - 480 °C
6.28 µin/in-°F
@Temperature 69.8 - 896 °F
Thermal Conductivity  25.3 W/m-K
@Temperature 20.0 °C
176 BTU-in/hr-ft²-°F
@Temperature 68.0 °F
 25.8 W/m-K
@Temperature 50.0 °C
179 BTU-in/hr-ft²-°F
@Temperature 122 °F
 27.0 W/m-K
@Temperature 100 °C
187 BTU-in/hr-ft²-°F
@Temperature 212 °F
 
Component Elements PropertiesMetricEnglishComments
Aluminum, Al 0.10 %0.10 %
Boron, B 0.0030 %0.0030 %
Carbon, C <= 0.030 %<= 0.030 %
Cobalt, Co 12 %12 %
Iron, Fe 63 %63 %As remainder
Manganese, Mn <= 0.10 %<= 0.10 %
Molybdenum, Mo 4.8 %4.8 %
Nickel, Ni 18.5 %18.5 %
Phosphorus, P <= 0.010 %<= 0.010 %
Silicon, Si <= 0.10 %<= 0.10 %
Sulfur, S <= 0.010 %<= 0.010 %
Titanium, Ti 1.4 %1.4 %
Zirconium, Zr 0.010 %0.010 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
AISI Grade 18Ni (350) Maraging Steel, Aged, at RT, tested longitudinal, round bar 16 mm
AISI Grade 18Ni (350) Maraging Steel nominal annealed properties
Sandvik 9RU10 Strip steel
AISI Grade 18Ni (350) Maraging Steel, Aged, at RT, tested longitudinal, round bar 32 mm
AISI Grade 18Ni (350) Maraging Steel, Aged, at RT, tested longitudinal, round bar 75 mm

M1835E / 7419

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.