MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Aptek 6110-A/B Epoxy Encapsulant and/or Potting Compound
Categories: Polymer; Thermoset; Epoxy; Epoxy Encapsulant, Unreinforced

Material Notes: Optoelectronic grade encapsulant/potting compound – will not attack/cloud polysulphone casings. More flexible, lower Tg version of APTEK 6106-A/B, for good temperature cycling in ceramic devices.

Part A is pale yellow to pale blue. Part B is water clear.

Information provided by Aptek Laboratories, Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.940 g/cc0.0340 lb/in³B Component; ASTM D1475
 1.15 g/cc0.0415 lb/in³A Component; ASTM D1475
Viscosity 65 cP65 cPB Component; Spindle #2; speed 100 rpm; ASTM D1824
 3400 cP3400 cPA Component; Spindle #3; speed 10 rpm; ASTM D1824
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 8585Cured property; ASTM D2240
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity >= 1.00e+15 ohm-cm>= 1.00e+15 ohm-cmCured property; ASTM D257
 
Thermal PropertiesMetricEnglishComments
Flash Point >= 100 °C>= 212 °FB Component; ASTM D92
 >= 200 °C>= 392 °FA Component; ASTM D92

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Tra-Con Tra-Cast 3113 General Purpose Epoxy Casting Compound
6110 Aluminum Composition Spec
Aptek 6106-A/B Epoxy Encapsulant and/or Potting Compound
BCC Products BC 9060 Silicone RTV Rubber
Aptek 6109-A/B Epoxy Encapsulant

PAPTEK41 / 24203

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.