MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

Braskem Green PE SLH218 Blow Film Extrusion and Cast Film Extrusion Linear Low Density Polyethylene
Categories: Polymer; Film; Renewable/Recycled Polymer; Thermoplastic; Polyethylene (PE); Linear Low Density (LLDPE); Linear Low Density Polyethylene (LLDPE), Film Grade

Material Notes: Description: SLH218 is a LLDPE Hexene copolymer produced by Braskem. It shows a good balance between optical properties, mechanical properties (Mainly stretchability), sealability and processability. Very low gel contained. The minimum biobased content of this grade is 84%, determined according to ASTM D6866.

Additive: Slip Absent; Antiblock Absent

Applications: Stretch films; Liners; LDPE and HDPE blends; packages for general use; Others applications: insulation for low and medium tension XLPE wires and cables; blends for irrigation pipes.

Information provided by Braskem.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 0.916 g/cc0.916 g/ccASTM D1505/D792
Thickness 25.0 microns0.984 mil
Melt Flow 2.3 g/10 min
@Load 2.16 kg,
Temperature 190 °C
2.3 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Film Elongation at Break, MD 1170 %1170 %ASTM D882
Film Elongation at Break, TD 1500 %1500 %ASTM D882
Elmendorf Tear Strength MD 240 g240 ggF; ASTM D1922
Elmendorf Tear Strength TD 520 g520 ggF; ASTM D1922
Dart Drop Test 110 g0.243 lbg/F50; ASTM D1709
Film Tensile Strength at Break, MD 40.0 MPa5800 psiASTM D882
Film Tensile Strength at Break, TD 40.0 MPa5800 psiASTM D882
1% Secant Modulus, MD 210 MPa30500 psiASTM D882
1% Secant Modulus, TD 240 MPa34800 psiASTM D882

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Braskem Green PE SLH118 Blow Film Extrusion and Cast Film Extrusion Linear Low Density Polyethylene
Braskem Green PE SLL118 Blow Film Extrusion and Cast Film Extrusion Linear Low Density Polyethylene
Braskem Green PE SLL318 Blow Film Extrusion and Cast Film Extrusion Linear Low Density Polyethylene
Braskem Green PE SBC818 Extrusion Coating Low Density Polyethylene
Braskem Green PE SBC818R50 Extrusion Coating Low Density Polyethylene

PBRAS707 / 109544

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.