MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Angst+Pfister APSOplast® PA 6 G MO PA 6 + molybdenum disulphide
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6); Nylon 6, MoS2 Filled

Material Notes: This cast polyamide contains finely distributed molybdenum disulphide particles which increase the crystallinity. This increases the mechanical properties as well as the friction and wear behavior without adversely affecting the high impact and fatigue resistance which are inherent to the non-modified cast polyamide 6 types. This material is used for various machine parts, plain bearings, sliding rails, gear wheels, idler pulleys, scrapers, chain sprockets, and pulleys.

Information provided by Angst + Pfister

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.15 g/cc0.0415 lb/in³DIN EN ISO 1183-1
Moisture Absorption 2.50 %2.50 %at saturation in standardized climate; DIN EN ISO 62
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 8383DIN EN ISO 868
Ball Indentation Hardness 185 MPa26800 psiDIN EN ISO 2039-1
Tensile Strength, Yield 82.0 MPa11900 psi50 mm/min; DIN EN ISO 527
Elongation at Break >= 35 %>= 35 %50 mm/min; DIN EN ISO 527
Modulus of Elasticity 3.50 GPa508 ksi1 mm/min; DIN EN ISO 527
Charpy Impact, Notched >= 0.250 J/cm²>= 1.19 ft-lb/in²DIN EN ISO 179-1eA
 
Thermal PropertiesMetricEnglishComments
CTE, linear 80.0 µm/m-°C
@Temperature 23.0 - 60.0 °C
44.4 µin/in-°F
@Temperature 73.4 - 140 °F
DIN 53752
Specific Heat Capacity 1.70 J/g-°C0.406 BTU/lb-°F
Thermal Conductivity 0.250 W/m-K1.74 BTU-in/hr-ft²-°F
Melting Point 216 °C421 °FISO 11357-3
Maximum Service Temperature, Air 110 °C230 °Fshort term
 170 °C338 °Flong term
Deflection Temperature at 1.8 MPa (264 psi) 95.0 °C203 °FDIN EN ISO 75/A
Minimum Service Temperature, Air -40.0 °C-40.0 °F
Flammability, UL94  HB
@Thickness 3.00 mm
HB
@Thickness 0.118 in
 HB
@Thickness 6.00 mm
HB
@Thickness 0.236 in
 
Descriptive Properties
Colorblack/anthracite

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PANGP032 / 250530

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.