MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

Haysite HCR-125 Vinyl Ester Sheet, Corrosion Resistant
Categories: Polymer; Thermoset; Vinyl Ester; Vinyl Ester Sheet Molding Compound

Material Notes: HCR-125 is a corrosion resistant vinyl ester sheet created by impregnating fiber glass mat, synthetic surface veil, and inert additives with Derkane 470 resin and catalyst. A compression molded product is produced by controlling a chemical reaction under heat and extreme pressure. Haysite HCR-125 offers excellent strength to weight ratios in addition to their corrosion resistance. Application: HCR-125 material can be sawed, sheared, machined, and punched to any size and shape. Successful applications include: tanks, tank covers, ductwork, exhaust and fume hoods, separators, bins, fan housings, trays, hoppers, sinks, lab table tops, fume scrubbers, heat exchanger plates, filter press plates, and other applications requiring a material with excellent resistance to corrosive elements. Standard color - Beige.

Information provided by Haysite

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.75 g/cc1.75 g/ccASTM D792
Water Absorption 0.20 %0.20 %ASTM D570
 
Mechanical PropertiesMetricEnglishComments
Hardness, Barcol 5454
Tensile Strength 74.5 MPa10800 psiASTM D638
Flexural Strength 167.0 MPa24220 psiASTM D790
Compressive Strength 241 MPa35000 psiASTM D695
Shear Strength 96.5 MPa14000 psiASTM D732
Izod Impact, Notched 5.13 J/cm9.60 ft-lb/inASTM D256
 
Electrical PropertiesMetricEnglishComments
Dielectric Strength 13.8 kV/mm350 kV/inPerpendicular in Oil; ASTM D149
Dielectric Breakdown 64000 V64000 VParallel, in Oil; ASTM D149
Arc Resistance 191 sec191 secASTM D495
 
Thermal PropertiesMetricEnglishComments
Flammability, UL94 V-0V-0
 
Descriptive Properties
Flame Resistance113 secondsIgnition Time, ASTM D229
 45 secondsBurning Time, ASTM D229

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
AR-Glass Fiber, Generic
Hexcel® HexForce™ 112 Fiber Glass Fabric
Mid-Mountain Materials PADMAT® MT1000 Needled Fiberglass Mat
PTS Trilac® ABS-GF3000-BK 30% Fiberglass Black ABS Resin
Fibre Glast 1110 L Vinyl Ester Resin (Laminate Properties)

PHAY518 / 142474

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.