MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Carmel Olefins Capilene® G 70 TF Polypropylene Homopolymer  (discontinued **)
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene, Sheet/Thermoforming Grade

Material Notes: Description: CAPILENE® G 70 TF is a nucleated polypropylene homopolymer intended for sheet extrusion and thermoforming applications. This grade exhibits high stiffness, high gloss, good contact transparency, short cycle time and improved characteristics at high temperature.

Applications: CAPILENE® G 70 TF is suitable for extrusion-thermoforming of thin, stiff and transparent food containers, containers for higher temperature filling.

Information provided by Carmel Olefins.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Melt Flow 3.0 g/10 min
@Load 2.16 kg,
Temperature 230 °C
3.0 g/10 min
@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 38.0 MPa5510 psi50 mm/min; ASTM D638
Elongation at Yield 9.0 %9.0 %50 mm/min; ASTM D638
Flexural Modulus 2.10 GPa305 ksiASTM D790
Izod Impact, Notched 0.300 J/cm0.562 ft-lb/inASTM D256
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 122 °C252 °FASTM D648
Vicat Softening Point 159 °C
@Load 1.02 kg
318 °F
@Load 2.25 lb
ASTM D1525
 
Optical PropertiesMetricEnglishComments
Haze 30 %
@Thickness 1.00 mm
30 %
@Thickness 0.0394 in
ASTM D1003
Transmission, Visible 90 %90 %transparent; thickness not quantified

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Overview of materials for Polypropylene with 10% Glass Fiber Filler
PolyMirae Moplen EP649N Polypropylene Copolymer
Total PPH 3429 Polypropylene, Injection Molding Grade
Hyosung Topilene J801 PP
Overview of materials for Polypropylene, Sheet/Thermoforming Grade

PCARM973 / 131148

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.