MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

AISI Type A11 Tool Steel (UNS T30111)
Categories: Metal; Ferrous Metal; Tool Steel; Air-Hardening Steel; Cold Work Steel

Material Notes: Air-Hardening Cold-Work Tool Steel. Applications: Punches and dies for blanking, piercing, cold heading and cold extrusions. Cold forming rolls. Knives for slitting, pelletizing and woodworking. Screws, nozzles and barrel liners for plastics compounding and injection molding. Powder metal compaction tooling.

Data provided by Bohler-Uddeholm and the references(s).

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 7.420 g/cc0.2681 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Hardness, Brinell 248 - 269248 - 269Annealed/Hardened
Modulus of Elasticity 221 GPa32100 ksi
 
Thermal PropertiesMetricEnglishComments
CTE, linear  10.7 µm/m-°C
@Temperature 20.0 - 93.0 °C
5.94 µin/in-°F
@Temperature 68.0 - 199 °F
 11.1 µm/m-°C
@Temperature 20.0 - 260 °C
6.17 µin/in-°F
@Temperature 68.0 - 500 °F
 11.8 µm/m-°C
@Temperature 20.0 - 427 °C
6.56 µin/in-°F
@Temperature 68.0 - 801 °F
 12.3 µm/m-°C
@Temperature 20.0 - 593 °C
6.83 µin/in-°F
@Temperature 68.0 - 1100 °F
Specific Heat Capacity 0.460 J/g-°C0.110 BTU/lb-°F
Thermal Conductivity  20.39 W/m-K
@Temperature 20.0 °C
141.5 BTU-in/hr-ft²-°F
@Temperature 68.0 °F
 21.54 W/m-K
@Temperature 100 °C
149.5 BTU-in/hr-ft²-°F
@Temperature 212 °F
 24.85 W/m-K
@Temperature 300 °C
172.5 BTU-in/hr-ft²-°F
@Temperature 572 °F
 26.3 W/m-K
@Temperature 500 °C
183 BTU-in/hr-ft²-°F
@Temperature 932 °F
 
Component Elements PropertiesMetricEnglishComments
Carbon, C 2.4 - 2.5 %2.4 - 2.5 %
Chromium, Cr 4.75 - 5.5 %4.75 - 5.5 %
Iron, Fe 78 - 81.4 %78 - 81.4 %As Balance
Manganese, Mn 0.35 - 0.60 %0.35 - 0.60 %
Molybdenum, Mo 1.1 - 1.5 %1.1 - 1.5 %
Phosphorus, P <= 0.030 %<= 0.030 %
Silicon, Si 0.75 - 1.1 %0.75 - 1.1 %
Sulfur, S 0.050 - 0.090 %0.050 - 0.090 %
Tungsten, W <= 0.50 %<= 0.50 %
Vanadium, V 9.25 - 10.25 %9.25 - 10.25 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
AISI Type A10 Tool Steel
Overview of materials for Air-Hardening Steel
Overview of materials for Cold Work Steel
AISI Type A2 Tool Steel
Overview of materials for Hot Work Steel

MSTA11 / 231067

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.