MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Mateck Thallium Bromoiodide TIBr-TII (KRS-5)
Categories: Ceramic; Halide

Material Notes: Optical crystals

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 7.371 g/cc0.2663 lb/in³
Solubility 0.050 ppm0.050 ppm
a Lattice Constant 0.4125 Å0.4125 Å
 
Mechanical PropertiesMetricEnglishComments
Vickers Microhardness 350350MPa
Modulus of Elasticity 31.0 GPa4500 ksi
Poissons Ratio 0.370.37
Shear Modulus 12.0 GPa1740 ksi
 
Thermal PropertiesMetricEnglishComments
CTE, linear 6.00 µm/m-°C
@Temperature 20.0 °C
3.33 µin/in-°F
@Temperature 68.0 °F
Specific Heat Capacity 0.151 J/g-°C0.0361 BTU/lb-°F
Thermal Conductivity 0.540 W/m-K
@Temperature 25.0 °C
3.75 BTU-in/hr-ft²-°F
@Temperature 77.0 °F
Melting Point 414.5 °C778.1 °F
 
Optical PropertiesMetricEnglishComments
Refractive Index 2.372.37at n10.0
 2.21
@Wavelength 40000 nm
2.21
@Wavelength 40000 nm
 2.29
@Wavelength 30000 nm
2.29
@Wavelength 30000 nm
 2.38
@Wavelength 4000 nm
2.38
@Wavelength 4000 nm
 2.60
@Wavelength 600 nm
2.60
@Wavelength 600 nm
Transmission, Visible  10 %
@Wavelength 650 nm
10 %
@Wavelength 650 nm
Internal Transmittance
 70 %
@Wavelength 670 nm
70 %
@Wavelength 670 nm
Internal Transmittance
IR Transmittance  10 %
@Wavelength 50000 nm
10 %
@Wavelength 50000 nm
Internal Transmittance
 72 %
@Wavelength 25000 nm
72 %
@Wavelength 25000 nm
Internal Transmittance
 
Descriptive Properties
Symmetrycubic
Symmetry Classm3m Pm3m
Transmission Range (microns)0.6 - 40

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Covestro Makrolon® 2408 Polycarbonate
Fused Quartz
Mateck Fused Silica UV-VIS Grade (SiO2)
Poco Graphite SUPERSiC® Basic Silicon Carbide
Covestro Makrolon® 1952 Polycarbonate

CMAT055 / 87739

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.