Afton plastics produces shapes and components from SABIC Ultem® 240 PEI, a high performance material that exhibits high strength and heat resistant properties. Glass-filled grades provide improved rigidity and dimensional stability. Product Benefits: UL 94 V-0 rating,• Microwave transparency • Temperature range: -4°F to +340°F • Withstands EtO, gamma radiation, autoclaving, and dry heat sterilization • Stable dielectric strength • Low thermal expansion • Low creep • Excellent hydrolytic and chemical stability. Applications: Fluid handling components, • Medical trays and instruments • Photographic lens housing • High heat test fixtures • Glass reinforced for high stiffness electrical housings • Aircraft and automotive parts • Food processing manifolds. Information provided by Afton Plastics. |