MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

Celanese Riteflex® XFR 440 TPC, Unfilled
Categories: Polymer; Thermoplastic; Polyester, TP; Polyester Thermoplastic Elastomer

Material Notes: Riteflex XFR 440 is a nominal 40 Shore D thermoplastic polyester elastomer featuring a halogen-free flame retardant system. It is UL certified to be V-0 at 1.5 mm in all colors. It exhibits an excellent balance of flexibility, flame redardance and processability.

Information provided by Celanese

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.20 g/cc0.0434 lb/in³ISO 1183
Melt Flow  7.1 g/10 min
@Load 2.16 kg,
Temperature 250 °C
7.1 g/10 min
@Load 4.76 lb,
Temperature 482 °F
ISO 1133
 15 g/10 min
@Load 2.16 kg,
Temperature 250 °C
15 g/10 min
@Load 4.76 lb,
Temperature 482 °F
[cm3/10min]; ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 404015 sec; ISO 868
Tensile Strength at Break 10.0 MPa1450 psi50mm/min; ISO 527-2/1A
Elongation at Break >= 50 %>= 50 %
 500 %500 %50mm/min; ISO 527-2/1A
Tensile Modulus 0.100 GPa14.5 ksi50mm/min; ISO 527-2/1A
Charpy Impact, Notched 2.50 J/cm²11.9 ft-lb/in²ISO 179/1eA
Tear Strength 40.0 kN/m228 pliISO 34-1
 
Electrical PropertiesMetricEnglishComments
Dielectric Strength 14.0 kV/mm356 kV/inIEC 60243-1
Comparative Tracking Index >= 600 V>= 600 VIEC 60112
 
Thermal PropertiesMetricEnglishComments
Melting Point 195 °C383 °F10°C/min; ISO 11357-1,-2,-3
Flammability, UL94 V-0
@Thickness 1.50 mm
V-0
@Thickness 0.0591 in
Oxygen Index 32.3 %32.3 %ISO 4589

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Celanese Riteflex® 655 Thermoplastic Polyester Elastomer (TPE)
Celanese Riteflex® XFR 655 TPC, Unfilled
Celanese Riteflex® 663 TPC, Unfilled
Celanese Riteflex® 677 TPC, Unfilled
Celanese Riteflex® UV655M TPC, Unfilled

PHCQ460 / 178915

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.