MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Hexcel® HexPly® F185 Epoxy Resin, 1581 Glass Fabric
Categories: Polymer; Thermoset; Epoxy; Epoxy/Glass SMC

Material Notes: Hexcel designation: 1581-38"-F185; Fiber: 150-1/2

Information provided by HexCel

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Filler Content 51.3 %51.3 %Laminate Fiber Volume
Volatiles 0.40 - 1.2 %0.40 - 1.2 %Prepreg
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield  2.779 MPa
@Temperature 82.0 °C
403.1 psi
@Temperature 180 °F
Flatwise TS
 5.537 MPa
@Temperature 24.0 °C
803.1 psi
@Temperature 75.2 °F
Flatwise TS
 8.432 MPa
@Temperature -54.0 °C
1223 psi
@Temperature -65.2 °F
Flatwise TS
 379 MPa
@Temperature 24.0 °C
55000 psi
@Temperature 75.2 °F
Warp TS
Compressive Yield Strength 345 MPa
@Temperature 24.0 °C
50000 psi
@Temperature 75.2 °F
Warp compression
Shear Strength  28.427 MPa
@Temperature 82.0 °C
4123.0 psi
@Temperature 180 °F
Lap shear
 31.778 MPa
@Temperature 24.0 °C
4609.0 psi
@Temperature 75.2 °F
Lap shear
 37.08 MPa
@Temperature -54.0 °C
5378 psi
@Temperature -65.2 °F
Lap shear
Peel Strength  8.24 kN/m
@Temperature -54.0 °C
47.0 pli
@Temperature -65.2 °F
Metal-to-metal
 11.1 kN/m
@Temperature 82.0 °C
63.3 pli
@Temperature 180 °F
Metal-to-metal
 12.8 kN/m
@Temperature 24.0 °C
73.0 pli
@Temperature 75.2 °F
Metal-to-metal
 
Descriptive Properties
Cured Thickness per Ply (cm)0.023Laminate
Flow (%)24-34
Wet Resin Content (%)47-53Prepreg

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Hexcel® HexPly® F650 Bismaleimide Resin with Fiberglass 7781 fabric reinforcement
Hexcel® HexPly® ES70 120°C Curing Epoxy Matrix, E-glass UD fabric 315 g/m2
Hexcel® F161 Epoxy Resin, 1581 Glass Fabric
Hexcel® HexPly® ES70 120°C Curing Epoxy Matrix, E-glass UD fabric 430 g/m2
Hexcel® HexPly® F155 Epoxy Resin, 1581 Glass Fabric

PHEXC115 / 98585

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.