MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Geon® Performance Solutions Vinyl Rigid Molding M3900 Polyvinyl Chloride, Rigid
Categories: Polymer; Thermoplastic; Vinyl (PVC); PVC, Rigid Grade

Material Notes:

Geon Performance Solutions was created from PolyOne in 2019.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.33 g/cc1.33 g/ccASTM D792
Linear Mold Shrinkage, Flow 0.0020 - 0.0050 cm/cm0.0020 - 0.0050 in/inASTM D955
Spiral Flow 88.9 cm35.0 in
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 7575ASTM D2240
Tensile Strength, Yield 37.9 MPa5500 psiType I, 51 mm/min; ASTM D638
Elongation at Break 60 %60 %Type I, 51 mm/min; ASTM D638
Tensile Modulus 2.28 GPa331 ksiType I, 51 mm/min; ASTM D638
Flexural Strength 65.5 MPa9500 psiASTM D790
Flexural Modulus 2.28 GPa331 ksiASTM D790
Izod Impact, Notched  2.10 J/cm
@Thickness 3.18 mm,
Temperature -18.0 °C
3.93 ft-lb/in
@Thickness 0.125 in,
Temperature -0.400 °F
Injection Molded; ASTM D256A
 5.90 J/cm
@Thickness 3.18 mm,
Temperature 0.000 °C
11.1 ft-lb/in
@Thickness 0.125 in,
Temperature 32.0 °F
Injection Molded; ASTM D256A
 7.50 J/cm
@Thickness 3.18 mm,
Temperature 23.0 °C
14.1 ft-lb/in
@Thickness 0.125 in,
Temperature 73.4 °F
Injection Molded; ASTM D256A
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi)  71.1 °C
@Thickness 6.35 mm
160 °F
@Thickness 0.250 in
Unannealed; ASTM D648
 77.2 °C
@Thickness 6.35 mm
171 °F
@Thickness 0.250 in
Annealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi)  70.0 °C
@Thickness 6.35 mm
158 °F
@Thickness 0.250 in
Unannealed; ASTM D648
 72.8 °C
@Thickness 6.35 mm
163 °F
@Thickness 0.250 in
Annealed; ASTM D648
UL RTI, Electrical 90.0 °C194 °FUL 746
UL RTI, Mechanical with Impact 85.0 °C185 °FUL 746
UL RTI, Mechanical without Impact 90.0 °C194 °FUL 746
Flammability, UL94  V-0
@Thickness 1.40 mm
V-0
@Thickness 0.0551 in
ALL; UL 94
 V-0
@Thickness 1.50 mm
V-0
@Thickness 0.0591 in
All Colors
 5VB
@Thickness 1.91 mm
5VB
@Thickness 0.0752 in
All Colors
 5VB
@Thickness 1.40 mm
5VB
@Thickness 0.0551 in
ALL; UL 94
 
Processing PropertiesMetricEnglishComments
Melt Temperature 199 - 210 °C390 - 410 °F
 
Descriptive Properties
FeaturesGeneral Purpose
 High Flow
 Low Temperature Impact Resistance
FormsPellets
Generic MaterialPVC, Rigid
Generic NamePolyvinyl Chloride, Rigid (PVC, Rigid)
Regional AvailabilityAfrica & Middle East
 Asia Pacific
 Europe
 North America
 South America
UsesAppliances
 Business Equipment
 Construction Applications
 Electrical/Electronic Applications
 General Purpose
 Telecommunications

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Geon® Performance Solutions Vinyl Fittings M1012 Polyvinyl Chloride, Rigid
Colorite Polymers 2002 Rigid PVC
Axiall 9109J Clear Rigid PVC, Extrusion, Clear
Geon® Performance Solutions Vinyl Rigid Extrusion 87555 Polyvinyl Chloride, Rigid
Geon® Performance Solutions 80510 Polyvinyl Chloride, Rigid

PH0POL0148 / 144717

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.