MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

Haysite ETR-FR-C Glass Reinforced Polyester Sheet, Electrical Grade (GPO3)
Categories: Polymer; Thermoset; Composite SMC; Filled/Reinforced Thermoset; Polyester, TS; Thermoset Polyester Glass SMC

Material Notes: ETR-FR-C meets NEMA GPO-3 requirements and exceeds NEMA in dielectric strength, arc resistance, and track resistance. This U.L. recognized grade is highly flame retardant and low smoke generating. ETR- FR-C is an IEEE 130ºC electrical/160ºC mechanical Class B material. Applications include high voltage appliance insulators, bus bar supports, and barriers in switchgear. Available in thicknesses .032" - 2.00". Standard color - Red. Meets Gov't Spec - I-24768/6.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.83 g/cc0.0661 lb/in³ASTM D572
Water Absorption 0.20 %0.20 %ASTM D570
 
Mechanical PropertiesMetricEnglishComments
Hardness, Barcol 6464
Tensile Strength, Ultimate 65.0 MPa9430 psi
Flexural Strength 145 MPa21000 psi
Flexural Modulus 11.0 GPa1600 ksi
Compressive Strength 241 MPa35000 psi
Shear Strength 97.0 MPa14100 psiASTM D732
Izod Impact, Notched 4.30 J/cm8.06 ft-lb/inedgewise; ASTM D256
 
Electrical PropertiesMetricEnglishComments
Dielectric Constant  4.69
@Frequency 1e+6 Hz
4.69
@Frequency 1e+6 Hz
ASTM D150
 4.73
@Frequency 60 Hz
4.73
@Frequency 60 Hz
ASTM D150
Dielectric Strength 18.0 kV/mm
@Thickness 1.59 mm
457 kV/in
@Thickness 0.0625 in
Perpendicular, Short Time in Oil and Air; ASTM D149
Dissipation Factor  0.011
@Frequency 1e+6 Hz
0.011
@Frequency 1e+6 Hz
ASTM D150
 0.016
@Frequency 60 Hz
0.016
@Frequency 60 Hz
ASTM D150
Arc Resistance 185 sec185 secASTM D495
Comparative Tracking Index >= 500 V>= 500 V
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 130 °C266 °FApproximate temperature class
Flammability, UL94 V-0V-0File No.E81893

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Haysite Ultratrac® H950 Glass Reinforced Polyester Sheet, Electrical Grade (GPO3)
Röchling Glastic Laminates/Shapes Polyester, Channels and Structural Shapes (GPO3)
AISI 1018 Steel, cold drawn
Haysite EHC Glass Reinforced Polyester Sheet, Electrical Grade (GPO1)
Haysite H722 Polyester, Glass Reinforced

PHAY17 / 45623

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.