Product Overview: LLF1019F6 is a general-purpose film grade linear low density made using the BP Gas Phase Process™ The resin exhibits excellent toughness and strength when drawn to thin gauges. Applications: - Blending resin
- Industrial packaging
- Industrial Liners
- Garment bags