MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

ITW Spraycore® SC 1800 LS Barrier Coat Vinyl Ester Syntactic Coring Material
Categories: Polymer; Thermoset; Vinyl Ester

Material Notes: The Spray core® line of sprayable syntactic materials and specialty sprayable fillers/primers. The Spray core® range of composite materials and sprayable industrial coatings have reengineered the boat building and composites industries. These sprayable laminates are lighter and stronger than hand-applied materials. SC 1800 LS is a sprayable premium vinyl ester barrier coat applied directly behind the gel coat. MEKP catalyst is not included. Product features: Outstanding performance when blocking skin coat print through. *Excellent gloss readings. *High Tensile elongation helps prevent gel coat stress cracking. *High resistance to water permeation. *Excellent flexural strength and fatigue resistance. Product benefits: Improves product cosmetics. *Helps increase blister resistance. *Reduces impact cracks. Preferred red dye catalyst: HP-90, DHD-9, MEKP 900.

Information provided by ITW Performance Polymers.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.743 - 0.815 g/cc0.0268 - 0.0294 lb/in³Application density
Viscosity 4000 - 7000 cP4000 - 7000 cPHB #4 @ 20 rpm
 
Chemical PropertiesMetricEnglishComments
Styrene Content 22 %22 %
 
Processing PropertiesMetricEnglishComments
Gel Time 3.00 - 5.00 min3.00 - 5.00 min
 3.00 - 7.00 min3.00 - 7.00 minGel to Peak
 
Descriptive Properties
ColorOff white/black
Laminate Skin Coat Application Interval25 to 40 min.
Peak Exotherm360 to 400°F100g mass
Thixotropy3.2 to 4.2

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PITWS9049 / 239559

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.