MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

Hexcel® HexPly® F650 Bismaleimide Resin with Graphite F3T584 fabric reinforcement
Categories: Polymer; Thermoset; Bismaleimide (BMI)

Material Notes: Aging Data, (T300-3K, 8 H.S.); Laminate Physicals: 59.6% Fiber volume, 34.0% Resin content, 1.0% Voids

Information provided by HexCel

Key Words: BMI
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesMetricEnglishComments
Flexural Yield Strength  655 MPa
@Temperature 232 °C
95000 psi
@Temperature 450 °F
Control (Prepreg with no freezer or out time exposure)
 710 MPa
@Temperature 232 °C
103000 psi
@Temperature 450 °F
Phase V (Prepreg stored in freezer 1 year at -9°C and exposed to 60 days at RT)
 731 MPa
@Temperature 232 °C
106000 psi
@Temperature 450 °F
Phase I (Prepreg stored in freezer 4 months at -9°C and exposed to 30 days at RT)
 758 MPa
@Temperature 232 °C
110000 psi
@Temperature 450 °F
Phase II (Prepreg stored in freezer 4 months at -9°C and exposed to 60 days at RT)
 814 MPa
@Temperature 232 °C
118000 psi
@Temperature 450 °F
Phase III (Prepreg stored in freezer 6 months at -9°C and exposed to 60 days at RT)
 827 MPa
@Temperature 232 °C
120000 psi
@Temperature 450 °F
Phase IV (Prepreg stored in freezer 1 year at -9°C and exposed to 30 days at RT)
 862 MPa
@Temperature 23.0 °C
125000 psi
@Temperature 73.4 °F
 869 MPa
@Temperature 23.0 °C
126000 psi
@Temperature 73.4 °F
 876 MPa
@Temperature 23.0 °C
127000 psi
@Temperature 73.4 °F
 889 MPa
@Temperature 23.0 °C
129000 psi
@Temperature 73.4 °F
 903 MPa
@Temperature 23.0 °C
131000 psi
@Temperature 73.4 °F
 924 MPa
@Temperature 23.0 °C
134000 psi
@Temperature 73.4 °F
Compressive Yield Strength  469 MPa
@Temperature 232 °C
68000 psi
@Temperature 450 °F
Phase II (Prepreg stored in freezer 4 months at -9°C and exposed to 60 days at RT)
 474 MPa
@Temperature 232 °C
68700 psi
@Temperature 450 °F
Phase V (Prepreg stored in freezer 1 year at -9°C and exposed to 60 days at RT)
 481 MPa
@Temperature 232 °C
69800 psi
@Temperature 450 °F
Phase III (Prepreg stored in freezer 6 months at -9°C and exposed to 60 days at RT)
 499 MPa
@Temperature 232 °C
72400 psi
@Temperature 450 °F
Phase IV (Prepreg stored in freezer 1 year at -9°C and exposed to 30 days at RT)
 532 MPa
@Temperature 232 °C
77200 psi
@Temperature 450 °F
Phase I (Prepreg stored in freezer 4 months at -9°C and exposed to 30 days at RT)
 558 MPa
@Temperature 232 °C
80900 psi
@Temperature 450 °F
Control (Prepreg with no freezer or out time exposure)
 606 MPa
@Temperature 23.0 °C
87900 psi
@Temperature 73.4 °F
 623 MPa
@Temperature 23.0 °C
90400 psi
@Temperature 73.4 °F
 703 MPa
@Temperature 23.0 °C
102000 psi
@Temperature 73.4 °F
 710 MPa
@Temperature 23.0 °C
103000 psi
@Temperature 73.4 °F
 731 MPa
@Temperature 23.0 °C
106000 psi
@Temperature 73.4 °F
 738 MPa
@Temperature 23.0 °C
107000 psi
@Temperature 73.4 °F
Shear Strength  44.3 MPa
@Temperature 232 °C
6430 psi
@Temperature 450 °F
Short Beam; Phase II (Prepreg stored in freezer 4 months at -9°C and exposed to 60 days at RT)
 45.9 MPa
@Temperature 232 °C
6660 psi
@Temperature 450 °F
Short Beam; Phase IV (Prepreg stored in freezer 1 year at -9°C and exposed to 30 days at RT)
 46.1 MPa
@Temperature 232 °C
6690 psi
@Temperature 450 °F
Short Beam; Phase I (Prepreg stored in freezer 4 months at -9°C and exposed to 30 days at RT)
 47.2 MPa
@Temperature 232 °C
6850 psi
@Temperature 450 °F
Short Beam; Phase V (Prepreg stored in freezer 1 year at -9°C and exposed to 60 days at RT)
 49.6 MPa
@Temperature 23.0 °C
7190 psi
@Temperature 73.4 °F
 51.1 MPa
@Temperature 232 °C
7410 psi
@Temperature 450 °F
Short Beam; Phase III (Prepreg stored in freezer 6 months at -9°C and exposed to 60 days at RT)
 51.7 MPa
@Temperature 232 °C
7500 psi
@Temperature 450 °F
Short Beam; Control (Prepreg with no freezer or out time exposure)
 55.2 MPa
@Temperature 23.0 °C
8010 psi
@Temperature 73.4 °F
 56.5 MPa
@Temperature 23.0 °C
8190 psi
@Temperature 73.4 °F
 60.7 MPa
@Temperature 23.0 °C
8800 psi
@Temperature 73.4 °F
 64.1 MPa
@Temperature 23.0 °C
9300 psi
@Temperature 73.4 °F
 68.7 MPa
@Temperature 23.0 °C
9960 psi
@Temperature 73.4 °F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Hexcel® HexFlow® RTM651 One-part Modified BMI Resin
Henkel Hysol EA 9833.1 (BMI) Core Splice Adhesive
Henkel Hysol EA 9673 (BMI) Film Adhesive
Evonik Compimide® TM124-ether 2,2'-Bis(4-allyloxyphenyl)propane
Evonik Compimide® TM124 2,2'-Bis(3-allyl-4-hydroxyphenyl)propane

PHEXC006 / 98476

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.