MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Daikin NEOFLON® EP-7000 Tubing Grade ETFE
Categories: Polymer; Thermoplastic; Fluoropolymer; ETFE/ECTFE; Fluorocarbon ETFE/ECTFE, Molded/Extruded

Material Notes: ETFE EP-7000 is a functionalized fluoropolymer specifically designed for the Automotive Industry. This resin has an excellent permeation resistance toward gasoline or flexible fuel and adheres well to many kinds of plastics without adhesive or etching. ETFE EP-7000 can be easily co-extruded into multilayer tubing and offers the following advantages for automotive applications. Excellent permeation resistance toward gasoline or flexible fuel. Increased temperature resistance Great chemical resistance. Co-extrusion with other resins (such as nylons, ETFE, EFEP, etc.) without adhesive or etching. Very good cold impact resistance. Superior bio-diesel compatibility

Information provided by Daikin.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.74 - 1.79 g/cc1.74 - 1.79 g/ccASTM D-792
Bulk Density >= 1.00 g/cc>= 0.0361 lb/in³
Melt Flow 18 - 23.2 g/10 min
@Temperature 297 °C
18 - 23.2 g/10 min
@Temperature 567 °F
ASTM D3159
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 30.0 - 50.0 MPa4350 - 7250 psiASTM D-3159
Elongation at Break >= 525 %>= 525 %ASTM D-3159
Compressive Yield Strength 10.7 MPa1550 psi1% Deformation; ASTM D695
Flex Crack Resistance 85008500Cycles per MIT Flex; ASTM D2176
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity >= 1.00e+17 ohm-cm>= 1.00e+17 ohm-cmASTM D257
Dielectric Constant  2.6
@Frequency 1000 Hz
2.6
@Frequency 1000 Hz
ASTM D150
 2.6
@Frequency 1e+6 Hz
2.6
@Frequency 1e+6 Hz
ASTM D150
Dielectric Strength 15.7 kV/mm
@Thickness 3.17 mm
400 kV/in
@Thickness 0.125 in
Short Time; ASTM D149
Dissipation Factor  0.00080
@Frequency 1000 Hz
0.00080
@Frequency 1000 Hz
ASTM D150
 0.0050
@Frequency 1e+6 Hz
0.0050
@Frequency 1e+6 Hz
ASTM D150
 
Thermal PropertiesMetricEnglishComments
Melting Point 251 - 259 °C484 - 498 °FASTM D3159
Maximum Service Temperature, Air 150 °C302 °FContinuous
Oxygen Index 31 %31 %ASTM D2863
 
Descriptive Properties
Permeation Resistance2.5 g.mm/m2.dayCE-10, 60°C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Daikin NEOFLON® RP-5000AS Tubing Grade EFEP
Daikin NEOFLON® EP-620 Extrusion/Molding Grade ETFE
Daikin NEOFLON® EP-610AS Extrusion/Molding Grade ETFE
Daikin NEOFLON® EP-610 Extrusion/Molding Grade ETFE
Daikin NEOFLON® EP-546 Extrusion Grade ETFE

PDAIJ9932 / 210003

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.