MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Daikin NEOFLON® AP-210AS PFA Pellets  (discontinued **)
Categories: Polymer; Thermoplastic; Fluoropolymer; Perfluoroalkoxy (PFA); Polyperfluoroalkoxyethylene, Molded/Extruded

Material Notes: NEOFLON PFA pellets have good melt flowability, and can be processed in the same manner as other thermoplastic resins.

Applications: Anti-static grader for injection molding.

Information provided by Daikin Industries.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 2.12 - 2.17 g/cc
@Temperature 25.0 °C
2.12 - 2.17 g/cc
@Temperature 77.0 °F
Bulk Density 1.20 g/cc0.0434 lb/in³
Water Absorption <= 0.010 %
@Thickness 8.50 mm,
Time 86400 sec
<= 0.010 %
@Thickness 0.335 in,
Time 24.0 hour
ASTM D570
Viscosity 1.00e+6 - 1.00e+7 cP
@Temperature 380 °C
1.00e+6 - 1.00e+7 cP
@Temperature 716 °F
Melt viscosity
Linear Mold Shrinkage 0.040 cm/cm0.040 in/in
Melt Flow 10 - 15 g/10 min
@Load 5.00 kg,
Temperature 372 °C
10 - 15 g/10 min
@Load 11.0 lb,
Temperature 702 °F
Deformation 2.4 %2.4 %6.7 MPa load, at 100°C, 24 hrs; ASTM D621
 2.7 %2.7 %13.7 MPa load, at 25°C, 24 hrs; ASTM D621
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 6060
Tensile Strength at Break 27.0 - 35.0 MPa3920 - 5080 psiASTM D638
Elongation at Break 280 - 400 %280 - 400 %ASTM D638
Tensile Modulus 0.451 GPa65.4 ksiASTM D638
Flexural Modulus 0.647 - 0.686 GPa93.8 - 99.5 ksiASTM D790
Compressive Strength 5.00 - 6.00 MPa
@Temperature 25.0 °C
725 - 870 psi
@Temperature 77.0 °F
1% deformation; ASTM D695
Izod Impact, Unnotched NBNBASTM D256
Coefficient of Friction 0.040 - 0.0600.040 - 0.060
Coefficient of Friction, Static 0.0500.050Coated-steel surface
Taber Abrasion, mg/1000 Cycles <= 96.75<= 96.759.8 N load, cs-10 wheel
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity <= 1.00e+18 ohm-cm<= 1.00e+18 ohm-cmASTM D257
Dielectric Constant  2.1
@Frequency 1000 Hz
2.1
@Frequency 1000 Hz
ASTM D150
 2.1
@Frequency 1e+6 Hz
2.1
@Frequency 1e+6 Hz
ASTM D150
Dielectric Strength 20.0 kV/mm
@Thickness 3.20 mm
508 kV/in
@Thickness 0.126 in
Short time; ASTM D149
Dissipation Factor  0.000010
@Frequency 1000 Hz
0.000010
@Frequency 1000 Hz
ASTM D150
 0.00030
@Frequency 1e+6 Hz
0.00030
@Frequency 1e+6 Hz
ASTM D150
 
Thermal PropertiesMetricEnglishComments
CTE, linear 120 µm/m-°C
@Temperature 23.0 - 60.0 °C
66.7 µin/in-°F
@Temperature 73.4 - 140 °F
ASTM D696
Melting Point 302 - 310 °C576 - 590 °F
Maximum Service Temperature, Air 260 °C500 °FContinuous use
Flammability, UL94 V-0V-0
Oxygen Index >= 95 %>= 95 %ASTM D2863
 
Descriptive Properties
Chemical ResistanceExcellent
Contact Angle115Angle to level
WeatherabilityExcellent

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Daikin NEOFLON® AP-201 PFA
Chemours 350 PFA Perfluoroalkoxy Copolymer
Zeus PFA Tubing and Drawn Fiber
Daikin NEOFLON® NF-0100 FEP Film
Daikin NEOFLON® EP-620AS Extrusion/Molding Grade ETFE

PDAIK110 / 29402

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.