MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Niagara LaSalle 4140 Leaded (41L40) Cold Finished Steel Bar
Categories: Metal; Ferrous Metal; Alloy Steel; AISI 4000 Series Steel

Material Notes: The addition of lead to this grade permits the production of some 25% more parts with excellent finish and good tool life. Machinability is raised to 145 sfm. Like 4140 annealed, it responds well to heat treatment with good strength and wear resistance, excellent toughness, good ductility in the quenched and tempered condition.

Information provided by Niagra LaSalle Corporation

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Component Elements PropertiesMetricEnglishComments
Carbon, C 0.38 - 0.43 %0.38 - 0.43 %
Chromium, Cr 0.80 - 1.1 %0.80 - 1.1 %
Iron, Fe 96.445 - 97.62 %96.445 - 97.62 %as balance
Lead, Pb 0.15 - 0.35 %0.15 - 0.35 %
Manganese, Mn 0.75 - 1.0 %0.75 - 1.0 %
Molybdenum, Mo 0.15 - 0.25 %0.15 - 0.25 %
Phosphorus, P <= 0.035 %<= 0.035 %
Silicon, Si 0.15 - 0.35 %0.15 - 0.35 %
Sulfur, S <= 0.040 %<= 0.040 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
AISI 4140 Steel, annealed at 815°C (1500°F) furnace cooled 11°C (20°F)/hour to 665°C (1230°F), air cooled, 25 mm (1 in.) round
Niagara LaSalle 4140 Cold Finished Steel Bar
AISI 4140 Steel, normalized at 870°C (1600°F), air cooled, 25 mm (1 in.) round
AISI 4140 Steel, normalized at 870°C (1600°F), air cooled, 13 mm (0.5 in.) round
Latrobe LSS™ 4140 Alloy Steel (AISI 4140)

NNIAL014 / 160304

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.