MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Materion Magnesium Fluoride MgF2 for Optical Coating
Categories: Ceramic; Halide

Material Notes: Materion has developed a manufacturing process for Magnesium Fluoride (MgF) which produces a highly pure, dense material form that is particularly well suited for optical coating. MgF, a low index coating material, has been used for many years in anti-reflection and multilayer coatings. It is insoluble and hard if deposited on hot substrates. Magnesium Fluoride evaporates cleanly and completely, without outgassing or spitting, and leaves a hard, uniform coating on the substrate.

Information provided by Materion.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Optical PropertiesMetricEnglishComments
Refractive Index  1.34
@Wavelength 1500 nm
1.34
@Wavelength 1500 nm
 1.35
@Wavelength 1000 nm
1.35
@Wavelength 1000 nm
 1.36
@Wavelength 700 nm
1.36
@Wavelength 700 nm
 1.365
@Wavelength 600 nm
1.365
@Wavelength 600 nm
 1.37
@Wavelength 500 nm
1.37
@Wavelength 500 nm
 1.375
@Wavelength 450 nm
1.375
@Wavelength 450 nm
 1.38
@Wavelength 400 nm
1.38
@Wavelength 400 nm
 1.39
@Wavelength 300 nm
1.39
@Wavelength 300 nm
 
Descriptive Properties
Evaporation Temperature950°C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

CMATER909 / 323521

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.