MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Silon Taborex TA 1134 HD Chemically-Crosslinkable HDPE Compound  (discontinued **)
Categories: Polymer; Thermoplastic; Polyethylene (PE); High Density (HDPE); High Density Polyethylene (HDPE), Crosslinkable (XLPE)

Material Notes: TABOREX TA 1134 HD is a crosslinkable compound made of Silane grafted ethylene polymer. This graft polymer constitutes together with a Masterbatch containing the crosslinking catalyst a “SIOPLAS-SYSTEM”. It is used for the production of single and multi-layer pipes for domestic hot and cold water, under floor heating and central heating application.

Information provided by Silon

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Bulk Density 0.550 g/cc0.0199 lb/in³DIN 53466
Density 0.943 g/cc0.0341 lb/in³DIN 53479/ASTM D1505
Volatiles <= 0.10 %<= 0.10 %ITM-ZP 300CH 3-5-5/d
Melt Flow 2.5 g/10 min
@Load 5.00 kg,
Temperature 190 °C
2.5 g/10 min
@Load 11.0 lb,
Temperature 374 °F
ISO 1133/ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 19.0 MPa2760 psiISO R 527
Elongation at Break 250 %250 %ISO R 527
 
Processing PropertiesMetricEnglishComments
Zone 1 160 - 170 °C320 - 338 °F
Zone 2 170 - 180 °C338 - 356 °F
Zone 3 170 - 190 °C338 - 374 °F
Zone 4 170 - 190 °C338 - 374 °F
Die Temperature 190 - 220 °C374 - 428 °F
Head Temperature 200 - 210 °C392 - 410 °F
Screw Cooling Temperature 70.0 - 90.0 °C158 - 194 °F
 
Descriptive Properties
Gel content (%)70EN 579

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Syensqo (Solvay Specialty Polymers) Polidan® T/A-SL Polyethylene, Crosslinked (XLPE)
Syensqo (Solvay Specialty Polymers) Polidan® T/A-MD Polyethylene, Crosslinked (XLPE)
Silon Taborex TA 1135 HD Chemically-Crosslinkable HDPE Compound
Overview of materials for High Density Polyethylene (HDPE), Crosslinkable

PSILON07 / 83545

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.