MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

Plenco 7467 Phenolic, Nodular, Transfer Molded  (discontinued **)
Categories: Polymer; Thermoset; Filled/Reinforced Thermoset; Phenolic; Phenolic, Novolac, Flock Filled

Material Notes: Two-Stage Phenolic. PLENCO 07467 is an organic phenolic molding compound offering excellent dimensional stability under conditions of total water immersion. 07467 is formulated to provide improved shock resistance and mechanical strength along with excellent dimensional stability. UL recognized under component file E40654. 07467 is available in black.

Information supplied by Plenco

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.45 g/cc0.0524 lb/in³ASTM D792
Apparent Bulk Density 0.550 g/cc0.0199 lb/in³Apparent density per ASTM D1895
Water Absorption 0.18 %0.18 %ASTM D570
Linear Mold Shrinkage 0.0050 cm/cm0.0050 in/inper ATM D955. Post shrinkage is 0.22% per ASTM D1299.
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell E 9191ASTM D785
Tensile Strength, Ultimate 50.8 MPa7370 psiASTM D638
Elongation at Break 0.75 %0.75 %ASTM D638
Tensile Modulus 7.85 GPa1140 ksiASTM D638
Flexural Yield Strength 76.4 MPa11100 psiASTM D790
Flexural Modulus 7.62 GPa1110 ksiASTM D790
Compressive Yield Strength 213 MPa30900 psiASTM D695
Poissons Ratio 0.350.35In tension
Shear Modulus 2.91 GPa422 ksiCalculated
Izod Impact, Notched 0.260 J/cm0.487 ft-lb/inASTM D256
Charpy Impact, Notched 0.300 J/cm²1.43 ft-lb/in²ASTM D256
Impact 153153J/m Plenco drop ball test
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 1.44e+11 ohm-cm1.44e+11 ohm-cmASTM D257
Dielectric Constant 5.8
@Frequency 1e+6 Hz
5.8
@Frequency 1e+6 Hz
ASTM D150
Dielectric Strength 8.80 kV/mm224 kV/inShort Time; ASTM D149
Dissipation Factor 0.071
@Frequency 1e+6 Hz
0.071
@Frequency 1e+6 Hz
ASTM D150
Arc Resistance 160 sec160 secASTM D495
Comparative Tracking Index 175 V175 VASTM D3638
 
Thermal PropertiesMetricEnglishComments
CTE, linear 35.0 µm/m-°C
@Temperature 20.0 °C
19.4 µin/in-°F
@Temperature 68.0 °F
Maximum Service Temperature, Air 200 °C392 °FHeat resistance per ASTM D794
Deflection Temperature at 1.8 MPa (264 psi) 183 °C361 °FASTM D648
Flammability, UL94 HB
@Thickness 1.47 mm
HB
@Thickness 0.0579 in

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PLEM38 / 50718

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.