MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Lehvoss LUVOCOM® 20/XCF/35/BK Polyphthalamide with carbon fiber  (discontinued **)
Categories: Polymer; Thermoplastic; Polyphthalamide (PPA); Polyphthalamide (PPA), Carbon Fiber Filled

Material Notes: Properties/attributes include: Very strong and stiff parts; low coefficient of thermal expansion. Electrically conductive, suitable for continuous discharging of statically-generated electricity. Low influence from moisture and temperature to measures and electrical properties, compared with PA66 Suitable for metal inserts.

Automotive industry, textile- and office machinery, apparatus- and precision engineering. Typical uses include: Bearings, sleeves, sliding elements, control disks, gear wheels, duty parts in switches.

Processing: During processing the moisture level should not exceed 0.05%, otherwise molecular degradation and surface defects (e.g. smearing) may occur. Processing temperatures above 340°C may very rapidly cause thermal damage and should therefore be avoided. The processing notes provided merely represent a recommendation for general use. Due to the large variety of machines, geometries and volumes of parts, etc., it may be necessary to employ different settings according to the specific application. High-temperature polymers place increased demands on the tool steels employed.

Information provided by Lehmann & Voss & Co.KG

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.35 g/cc1.35 g/ccISO 1183
Moisture Absorption <= 0.300 %
@Temperature 23.0 °C,
Time 86400 sec
<= 0.300 %
@Temperature 73.4 °F,
Time 24.0 hour
Linear Mold Shrinkage <= 0.0010 cm/cm<= 0.0010 in/inDIN 16901
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength 386 MPa56000 psiISO 527-2
Elongation at Break 1.5 %1.5 %ISO 527-2
Modulus of Elasticity 36.0 GPa5220 ksiISO 527-2
Flexural Strength 527 MPa76400 psiISO 178
Flexural Modulus 31.0 GPa4500 ksiISO 178
Flexural Strain at Break 2.0 %2.0 %Flexural Elongation @ Fmax; ISO 178
Charpy Impact Unnotched 8.30 J/cm²
@Temperature 23.0 °C
39.5 ft-lb/in²
@Temperature 73.4 °F
ISO 179 1eU
Charpy Impact, Notched 0.900 J/cm²
@Temperature 23.0 °C
4.28 ft-lb/in²
@Temperature 73.4 °F
ISO 179 1eA
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity <= 1000 ohm-cm<= 1000 ohm-cmIEC 60167
Surface Resistance <= 1000 ohm<= 1000 ohmIEC 60093
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 165 °C329 °FContinuous; UL 746B
 195 °C383 °FShort Term
Deflection Temperature at 1.8 MPa (264 psi) 270 °C518 °FISO 75-2/A
 
Processing PropertiesMetricEnglishComments
Nozzle Temperature 315 - 335 °C599 - 635 °F
Zone 1 300 - 320 °C572 - 608 °F
Zone 2 310 - 330 °C590 - 626 °F
Zone 3 315 - 335 °C599 - 635 °F
Melt Temperature 320 °C608 °F
Mold Temperature 135 - 160 °C275 - 320 °F
Drying Temperature  80.0 °C
@Time >=57600 sec
176 °F
@Time >=16.0 hour
Dehumidifying dryer
 105 °C
@Time 14400 - 18000 sec
221 °F
@Time 4.00 - 5.00 hour
Vacuum Dryer
Moisture Content <= 0.050 %<= 0.050 %
 
Descriptive Properties
Colorblack

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Overview of materials for 6000 Series Aluminum Alloy
Overview of materials for Polyphthalamide (PPA), Carbon Fiber
RTP Company RTP 4087 Polyphthalamide (PPA); Carbon Fiber
Nurel Engineering Polymers Promyde® B30 P2 G40 MI PA 6, Dry, 40% Glass Reinforced, Injection Molded, Impact modified and Heat Stabilized
Lehvoss LUVOCOM® 50/GF/20/TF/20/BK 100 Polycarbonate with glass fiber and PTFE

PLUU8906 / 193865

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.