MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Schott BG3 Band Pass Filter
Categories: Ceramic; Glass; Optical; Filter

Material Notes: Ionically colored glass. Data provided by the manufacturer, Schott Glas Mainz.

Key Words: DIN BP 368/185
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 2.56 g/cc0.0925 lb/in³
 
Chemical PropertiesMetricEnglishComments
Acid Class, SR 11
Alkali Class, AR 11
Stain Resistance Class, FR 0.00.0
 
Thermal PropertiesMetricEnglishComments
CTE, linear  8.80 µm/m-°C
@Temperature -30.0 - 70.0 °C
4.89 µin/in-°F
@Temperature -22.0 - 158 °F
 10.2 µm/m-°C
@Temperature 20.0 - 300 °C
5.67 µin/in-°F
@Temperature 68.0 - 572 °F
Transformation Temperature, Tg 478 °C892 °F
 
Optical PropertiesMetricEnglishComments
Refractive Index  1.50
@Wavelength 1014 nm
1.50
@Wavelength 1014 nm
Hg
 1.51
@Wavelength 587.6 nm
1.51
@Wavelength 587.6 nm
He
 1.52
@Wavelength 435.8 nm
1.52
@Wavelength 435.8 nm
Hg
 1.55
@Wavelength 302.1 nm
1.55
@Wavelength 302.1 nm
Hg
Transmission, Visible  <= 1.0 %
@Wavelength 510 - 6801 nm
<= 1.0 %
@Wavelength 510 - 6801 nm
 87 %
@Wavelength 400 nm
87 %
@Wavelength 400 nm
Internal transmittance of 95% at 400 nm
IR Transmittance 91 %
@Wavelength 750 - 900 nm
91 %
@Wavelength 750 - 900 nm
Internal transmittance of 99% from 750-900 nm.
UV Transmittance  <= 0.0060 %
@Wavelength 200 - 250 nm
<= 0.0060 %
@Wavelength 200 - 250 nm
 91 %
@Wavelength 340 - 370 nm
91 %
@Wavelength 340 - 370 nm
Internal transmittance of 99% from 340-370 nm
Reflection Coefficient, Visible (0-1) 0.92
@Wavelength 587.6 nm
0.92
@Wavelength 587.6 nm
Reflection Factor P

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
AISI 1045 Steel, cold drawn, 19-32 mm (0.75-1.25 in) round
AISI 1010 Steel, CQ sheet,1.6-5.8 mm round or thickness
AISI 1045 Steel, Quenched and Tempered to 595 HB
Industeel CREUSABRO® M Wear Resistant Steel
AISI 1015 Steel, hot rolled, 19-32 mm (0.75-1.25 in) round

CSGT01 / 1990

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.