MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Barlog Plastics KEBABLEND M 15/19 PPS for Plastic Bonded Magnets
Categories: Polymer; Thermoplastic; Polyphenylene Sulfide (PPS); Polyphenylene Sulfide (PPS) with 10% Carbon Fiber Filler

Material Notes: PPS functional compound for the production of plastic bonded magnets

Properties: dimensionally stable, high continuous used temperature, magnetizable

Typical areas of application: Holding magnets, Magnets for sensors, Pumps and motors

Industries: Automotive, Electrical and electronics industry, Household appliances, Mechanical Engineering

Information provided by BARLOG plastics GmbH.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 3.74 g/cc0.135 lb/in³ISO 1183-1
Linear Mold Shrinkage, Flow 0.00600 cm/cm0.00600 in/inISO 294-4
Linear Mold Shrinkage, Transverse 0.00600 cm/cm0.00600 in/inISO 294-4
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 60.0 MPa8700 psiISO 527-1
Elongation at Break 2.00 %2.00 %ISO 527-1
Modulus of Elasticity 31.0 GPa4500 ksiISO 527-1
 
Electrical PropertiesMetricEnglishComments
Magnetic Coercive Force, Hc 2450 Oe2450 Oe195 kA/m; DIN EN 60404-5
Magnetic Remanence, Br 2750 Gauss2750 Gauss275 mT; DIN EN 60404-5
Magnetic Maximum Energy Product, BH 1.88 MGOe1.88 MGOe15 kJ/m³; DIN EN 60404-5
 
Thermal PropertiesMetricEnglishComments
Melting Point 285 °C545 °FISO 11357-1/-3
 
Processing PropertiesMetricEnglishComments
Melt Temperature 300 - 330 °C572 - 626 °F
Mold Temperature 140 - 160 °C284 - 320 °F
Drying Temperature 120 °C248 °F
Dry Time 4.00 - 8.00 hour4.00 - 8.00 hour
Back Pressure 4.00 - 8.00 MPa580 - 1160 psi
 
Descriptive Properties
Magnetic properties15 kJ/m³max. energy product (BH max), DIN EN 60404-5

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PBARLO429 / 326503

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.