MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Desktop Metal 17-4 PH Shop System™ Stainless Steel; 3D Printed, As-Sintered
Categories: Metal; 3D Printing/Additive Manufacturing Metal; Ferrous Metal; Stainless Steel; Precipitation Hardening Stainless

Material Notes: 17-4 PH 3D Printed Stainless steel is an excellent material with great mechanical properties, long lifetime, high hardness, and mild corrosion resistance. This metal alloy is the perfect choice for the traditional operating environments of a manufacturing floor. It can be heat-treated to a variety of hardness and toughness levels, allowing users to customize the post-sintering properties in order to suit a wide variety of applications.

Applications

  • Manufacturing Machinery
  • Pump Components
  • Chemical Processing
  • Valving, Fasteners
  • Food Processing
  • Jigs and Fixtures

Information provided by Proto3000

Key Words: Metal Binder Jetting, UNS S17400, EN 1.4542, ISO 4542-174-00-I
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 7.50 - 7.66 g/cc0.271 - 0.277 lb/in³ASTM B311
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell C 25.4 - 27.425.4 - 27.4ASTM E18
Tensile Strength, Ultimate 877 - 947 MPa127000 - 137000 psiASTM E8M
Tensile Stress  200 MPa
@Strain 0.1 %
29000 psi
@Strain 0.1 %
 800 MPa
@Strain 0.9 %
116000 psi
@Strain 0.9 %
 950 MPa
@Strain 1.5 %
138000 psi
@Strain 1.5 %
Tensile Strength, Yield 620 - 700 MPa89900 - 102000 psiASTM E8M
Elongation at Break 3.90 - 7.90 %3.90 - 7.90 %ASTM E8M
Modulus of Elasticity 148 - 208 GPa21500 - 30200 ksiASTM E8M
 
Component Elements PropertiesMetricEnglishComments
Carbon, C <= 0.0700 %<= 0.0700 %
Chromium, Cr 15.5 - 17.5 %15.5 - 17.5 %
Copper, Cu 3.00 - 5.00 %3.00 - 5.00 %
Iron, Fe 69.98 - 78.35 %69.98 - 78.35 %Balance
Manganese, Mn <= 1.00 %<= 1.00 %
Nb + Ta 0.150 - 0.450 %0.150 - 0.450 %
Nickel, Ni 3.00 - 5.00 %3.00 - 5.00 %
Silicon, Si <= 1.00 %<= 1.00 %
 
Descriptive Properties
Surface Roughness4.1xy (µm Ra), @ 75 ?m Layer Thickness
 8z (µm Ra), @ 75 ?m Layer Thickness

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

NPROTO875 / 322888

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.