MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

LyondellBasell Purell PE 2420 F Low Density Polyethylene (LDPE)
Categories: Polymer; Film; Thermoplastic; Polyethylene (PE); Low Density (LDPE); Low Density Polyethylene (LDPE), Blow Molding Grade

Material Notes: Purell PE 2420F is a high purity low density polyethylene with good processability, good optical and good chemical resistance. It is delivered in pellet form. The grade is used for films for healthcare applications including packaging of pharmaceuticals. Applications: Bags & Pouches, Blow-Fill-Seal Applications, Healthcare Applications, Medical Devices, Medical Film, Secondary Packaging.

Information provided by LyondellBasell.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.923 g/cc0.0333 lb/in³ISO 1183-1
Melt Flow 0.75 g/10 min
@Load 2.16 kg,
Temperature 190 °C
0.75 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ISO 1133-1
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 4848ISO 868
Ball Indentation Hardness 18.0 MPa2610 psiISO 2039-1
Tensile Strength, Yield 11.0 MPa1600 psiISO 527-1,-2
Film Elongation at Break, MD 300 %300 %ISO 527-1,-3
Film Elongation at Break, TD 600 %600 %ISO 527-1,-3
Tensile Modulus 0.260 GPa37.7 ksiISO 527-1,-2
Film Tensile Strength at Break, MD 26.0 MPa3770 psiISO 527-1,-3
Film Tensile Strength at Break, TD 20.0 MPa2900 psiISO 527-1,-3
 
Thermal PropertiesMetricEnglishComments
Melting Point 111 °C232 °FDSC; ISO 3146
Vicat Softening Point 96.0 °C205 °FA50N; ISO 306
 
Descriptive Properties
Processing MethodBlow, Fill, & Seal, Blown Film, Extrusion Blow Molding, Injection Blow Molding

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Braskem HB 0155 HDPE Blow Molding Polyethylene
Amco PRIMATOP HDPE 003946HP Blow Molding Polyethylene
LyondellBasell Purell PE1840H Low Density Polyethylene, Blown Film, Injection Molding, Blow Fill & Seal, Extrusion Blow Molding
Overview of materials for High Density Polyethylene (HDPE), Blow Molding Grade
A. Schulman LP477-01 High-Density Polyethylene

PEQT8633 / 220267

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.