MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Carlson 2205 (UNS S31803) Duplex Stainless Steel
Categories: Metal; Ferrous Metal; Austenitic; Duplex; Stainless Steel

Material Notes: General Description

Carlson Alloy 2205 is a second-generation, nitrogen-alloyed duplex stainless steel (ferritic-austenitic). It offers an excellent combination of both strength and corrosion resistance over a wide range of applications. The approximate 50/50 ferrite-austenite structure provides excellent chloride pitting and stress corrosion cracking resistance, with roughly twice the yield strength of the standard austenitic stainless grades.

The high chromium and molybdenum content, coupled with the nitrogen addition in 2205, provides general corrosion, pitting, and crevice corrosion resistance superior to 316L and 317L.

2205 demonstrates superior erosion-corrosion resistance when compared to 316 stainless steel. It is not subject to intergranular corrosion in the as-welded condition. 2205 may be successfully machined by conventional methods.

The (UNS S32205) grade is a restricted-chemistry version which maintains chromium, molybdenum and nitrogen at higher levels than the (UNS S31803) composition.

Applications

Due to its excellent corrosion resistance, 2205 is a suitable material for service in environments containing chlorides and hydrogen sulfide. It is also suitable foe use in dilute sulfuric acid solutions and for handling organic acids, i.e., acetic acid and its mixtures.

  • Oil and Gas Production – Down-hole piping, gathering line pipe, CO2 tertiary recovery piping, oil-gas separators, heat exchangers.
  • Chemical Processing – Heat exchangers, pressure vessels, tanks, columns, pumps, valves, piping.
  • Transportation – Tank trailers, ocean-going tankers, barges.
  • Pulp & Paper – Pulp digesters
  • Power Industry – Feedwater heaters, coolers, flue gas scrubbers.
  • Marine Service – Sea water piping, pumps.

Information provided by Carlson

Key Words: UNS S31803
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 7.82 g/cc0.283 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Hardness, Brinell <= 293<= 293
Hardness, Rockwell C <= 31<= 31
Tensile Strength at Break >= 621 MPa>= 90000 psi
Tensile Strength, Yield >= 448 MPa
@Strain 0.2 %
>= 65000 psi
@Strain 0.2 %
Elongation at Break >= 25 %>= 25 %
Modulus of Elasticity 190 GPa27500 ksi
 
Thermal PropertiesMetricEnglishComments
CTE, linear  13.7 µm/m-°C
@Temperature 20.0 - 100 °C
7.60 µin/in-°F
@Temperature 68.0 - 212 °F
 14.2 µm/m-°C
@Temperature 20.0 - 199 °C
7.90 µin/in-°F
@Temperature 68.0 - 390 °F
 14.8 µm/m-°C
@Temperature 20.0 - 299 °C
8.20 µin/in-°F
@Temperature 68.0 - 570 °F
Specific Heat Capacity 0.418 J/g-°C
@Temperature 20.0 °C
0.100 BTU/lb-°F
@Temperature 68.0 °F
 
Component Elements PropertiesMetricEnglishComments
Carbon, C <= 0.030 %<= 0.030 %
Chromium, Cr 21 - 23 %21 - 23 %
Iron, Fe 63.75 - 71.92 %63.75 - 71.92 %
Manganese, Mn <= 2.0 %<= 2.0 %
Molybdenum, Mo 2.5 - 3.5 %2.5 - 3.5 %
Nickel, Ni 4.5 - 6.5 %4.5 - 6.5 %
Nitrogen, N 0.080 - 0.20 %0.080 - 0.20 %
Phosphorus, P <= 0.030 %<= 0.030 %
Silicon, Si <= 1.0 %<= 1.0 %
Sulfur, S <= 0.020 %<= 0.020 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Carlson 2205 (UNS S32205) Duplex Stainless Steel
AK Steel 2205 Duplex Stainless steel
Outokumpu 2205 Duplex Stainless Steel
MetalTek MTEK 2205 Cast UNS J92205 Duplex Stainless Steel
Industeel URANUS® 45N 22Cr 3Mo Duplex Stainless Steel with PREN = 33 or 34

NCARLSO10 / 15817

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.