MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Titanium Ti-8V-5Fe-1Al, Annealed
Categories: Metal; Nonferrous Metal; Titanium Alloy; Beta Titanium Alloy

Material Notes: Annealed: 675 °C, 1/2 hour, air cooled.

Characteristics: Metastable beta alloy, very high tensile and shear strengths.

Applications: Aerospace fasteners.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 4.65 g/cc0.168 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Hardness, Vickers 330330after undergoing deformation at 850 °C
Tensile Strength 1263 MPa183200 psi
Tensile Strength, Yield 1233 MPa178800 psi
Elongation at Break 15 %15 %
Reduction of Area 47.5 %47.5 %
Tensile Modulus 114 GPa16500 ksi
 101 GPa
@Temperature 315 °C
14600 ksi
@Temperature 599 °F
 
Component Elements PropertiesMetricEnglishComments
Aluminum, Al 0.80 - 1.5 %0.80 - 1.5 %
Carbon, C <= 0.050 %<= 0.050 %
Iron, Fe 4.0 - 6.0 %4.0 - 6.0 %
Nitrogen, N <= 0.070 %<= 0.070 %
Oxygen, O 0.25 - 0.50 %0.25 - 0.50 %
Titanium, Ti 86 %86 %
Vanadium, V 7.5 - 8.5 %7.5 - 8.5 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Titanium Ti-15Mo-5Zr-3Al Duplex Aged
Touchstone MetPreg™ Fiber Reinforced Aluminum
Titanium Ti-8V-5Fe-1Al, STA
Titanium Beta-21S (Grade 21)
Titanium Ti-13V-11Cr-3Al; (Ti-13-11-3) Annealed 850°C (1560°F) + Aged 510°C 8 hr

MTB851 / 142964

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.