MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

AK Steel 17-7 PH® Precipitation Hardening Stainless Steel, Condition A
Categories: Metal; Ferrous Metal; Austenitic; Stainless Steel; Precipitation Hardening Stainless

Material Notes: AK Steel 17-7 PH® provides high strength and hardness, excellent fatigue properties, good corrosion resistance, good formability, and minimum distortion upon heat treatment. This alloy provides valuable property combinations particularly well suited for aerospace applications. This special alloy also provides benefits for other applications requiring high strength and good corrosion resistance, as well as excellent properties for flat springs at temperatures up to 600°F (310°C).

The material supplied from the mill is in Condition A. After fabrication, and conditioning treatments, the material is precipitation hardened into either Condition TH 1050 or Condition RH 950. To achieve the highest mechanical properties Condition A material is transformed to martensite at the mill by cold reduction to Condition C. After fabrication by the user a single low-temperature heat treatment is preformed to achieve condition CH 900.

Information provided by AK Steel

Key Words: UNS S17700
Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 7.81 g/cc0.282 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell B 8585
Tensile Strength, Ultimate 896 MPa130000 psi
Tensile Strength, Yield 276 MPa
@Strain 0.2 %
40000 psi
@Strain 0.2 %
Elongation at Break 35 %35 %in 2 inches
Modulus of Elasticity 200 GPa29000 ksi
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.0000800 ohm-cm0.0000800 ohm-cm
Magnetic Permeability 1.4 - 3.21.4 - 3.2200 Oersted
 1.4 - 3.61.4 - 3.6maximum
 1.4 - 3.61.4 - 3.650 Oersted
 
Thermal PropertiesMetricEnglishComments
CTE, linear  15.3 µm/m-°C
@Temperature 21.0 - 93.0 °C
8.50 µin/in-°F
@Temperature 69.8 - 199 °F
 16.0 µm/m-°C
@Temperature <=427 °C
8.89 µin/in-°F
@Temperature <=801 °F
 
Component Elements PropertiesMetricEnglishComments
Aluminum, Al 0.75 - 1.5 %0.75 - 1.5 %
Carbon, C <= 0.090 %<= 0.090 %
Chromium, Cr 16 - 18 %16 - 18 %
Iron, Fe 70.59 - 76.75 %70.59 - 76.75 %As Remainder
Manganese, Mn <= 1.0 %<= 1.0 %
Nickel, Ni 6.5 - 7.75 %6.5 - 7.75 %
Phosphorus, P <= 0.040 %<= 0.040 %
Silicon, Si <= 1.0 %<= 1.0 %
Sulfur, S <= 0.030 %<= 0.030 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
AK Steel 17-4 PH® Precipitation Hardening Stainless Steel, Condition H 900
AK Steel 17-4 PH® Precipitation Hardening Stainless Steel, Condition A
AK Steel 17-4 PH® Precipitation Hardening Stainless Steel, Condition H 925
AK Steel 17-7 PH® Precipitation Hardening Stainless Steel, Condition RH 950
AK Steel 17-7 PH® Precipitation Hardening Stainless Steel, Condition CH 900

NAKS135 / 14738

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.