MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Dow 500.00 Performance Polypropylene Polymer  (discontinued **)
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene, Sheet/Thermoforming Grade

Material Notes: D 500.00 Developmental Performance Polymer is a performance plastic designed for cut sheet thermoforming. The propylene-based polymer offers improved formability in large part thermoforming applications.

    Main Characteristics
  • Melt strength specifically suited to the thermoforming process
  • Improved sheet sag / drape performance
  • Low temperature toughness
  • High chemical resistance
  • Better regrind capability without significant loss of properties

Braskem acquired Dow's polypropylene business. This specific grade was discontinued priot to the acquisition and so is listed as a discontinued Dow product.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.13 g/cc0.0408 lb/in³ASTM D792
Melt Index of Compound 0.45 g/10 min
@Load 2.16 kg,
Temperature 230 °C
0.45 g/10 min
@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 19.3 MPa2800 psiASTM D638
Elongation at Yield 4.0 %4.0 %ASTM D638
Flexural Modulus 2.00 GPa290 ksiTangent; ASTM D790A
Izod Impact, Notched  1.07 J/cm
@Temperature -18.0 °C
2.00 ft-lb/in
@Temperature -0.400 °F
ASTM D256
 5.87 J/cm
@Temperature 23.0 °C
11.0 ft-lb/in
@Temperature 73.4 °F
ASTM D256
Dart Drop, Total Energy  21.0 J
@Temperature 23.0 °C
15.5 ft-lb
@Temperature 73.4 °F
Peak Energy; ASTM D3763
 30.7 J
@Temperature -18.0 °C
22.6 ft-lb
@Temperature -0.400 °F
Peak Energy; ASTM D3763
 
Thermal PropertiesMetricEnglishComments
CTE, linear 40.0 µm/m-°C
@Temperature -30.0 - 30.0 °C
22.2 µin/in-°F
@Temperature -22.0 - 86.0 °F
ASTM D696
Deflection Temperature at 0.46 MPa (66 psi) 110 °C230 °FUnannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 58.3 °C137 °FUnannealed; ASTM D648
 
Optical PropertiesMetricEnglishComments
Gloss >= 80 %>= 80 %ASTM D523; 60°, Thermoformed
 90 %90 %ASTM D523; 60°, Extruded Sheet

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
MTM Plastics Purpolen® PP Polypropylene Regrind
Dow 560.01 Performance Polypropylene Polymer
Rogers Arlon AD300C Commercial Microwave and RF Laminate Material
Rogers Arlon MULTICLAD™ HF Halogen-Free Low-Loss Laminate and Prepreg System
Dow R131-02A Polypropylene Random Copolymer Resin

PDOW0991 / 93327

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.