MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

LATI Latene® AG3H GS/40 40% Mixed Chemically Coupled Glass Spheres and Fibers, Heat-Stabilized Polypropylene Homopolymer (PPH)  (discontinued **)
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene with Glass Fiber + Bead Filler

Material Notes: Description: Latene series thermoplastics are polypropylene homopolymer (PPH) products. They provide good mechanical, thermal and electrical properties together with good chemical inertness. The wide range of filled Latene allows a choice based on shrinkage, impact resistance, rigidity and/or surface finish, according to project demands. Compared to filled versions, reinforced Latene grades, especially chemically coupled versions, offer considerably greater rigidity and thermal resistance under loads. All the Latene grades may be adapted to specific project needs. Several characteristics may be enhanced, such as flowability, heat-stability, anti-static quality, stability on contact with metals and detergents, UV-stabilization (except for normal self-extinguishing types).

Specific Notes for this Material: 40% mixed chemically coupled glass spheres and fibers; heat-stabilized; good dimensional stability.

Disclaimer from LATI: This document contains information based on average values as obtained from the results of laboratory tests and observations made on LATI materials. Tested materials were injection molded, used in their natural color, and conditioned in compliance with Standard ASTM D 618, procedure A. These values refer to LATI's best technical and scientific knowledge at the moment of testing and cannot be used as a basis for the development of applications. For a better assessment of the materials, you are kindly requested to contact LATI's technical or commercial offices, which are at your disposal and will supply detailed information on the most suitable characteristics for their intended use. With reference to DPR n.224 dated May 24, 1988, issued in accordance with EC Guide-lines 85/374, LATI Industria Termoplastici S.p.A. declines all responsibility arising from an improper use of the products described in this document.

All data provided by LATI.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.20 g/cc0.0434 lb/in³ISO 1183
Water Absorption 0.020 %0.020 %at 23°C; ISO 62
Linear Mold Shrinkage 0.0030 cm/cm0.0030 in/inLATI
Linear Mold Shrinkage, Transverse 0.0080 cm/cm0.0080 in/inLATI
Melt Flow 2.5 g/10 min2.5 g/10 minISO 1133
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell M 7373ASTM D785
Tensile Strength, Ultimate 62.0 MPa8990 psiISO 527
 18.0 MPa
@Temperature 120 °C
2610 psi
@Temperature 248 °F
ISO 527
 30.0 MPa
@Temperature 90.0 °C
4350 psi
@Temperature 194 °F
ISO 527
 40.0 MPa
@Temperature 60.0 °C
5800 psi
@Temperature 140 °F
ISO 527
Flexural Modulus 4.80 GPa696 ksiASTM D790
 1.95 GPa
@Temperature 120 °C
283 ksi
@Temperature 248 °F
ASTM D790
 2.57 GPa
@Temperature 90.0 °C
373 ksi
@Temperature 194 °F
ASTM D790
 3.25 GPa
@Temperature 60.0 °C
471 ksi
@Temperature 140 °F
ASTM D790
Izod Impact, Notched  0.400 J/cm
@Temperature -40.0 °C
0.749 ft-lb/in
@Temperature -40.0 °F
ASTM D256
 0.450 J/cm
@Temperature -20.0 °C
0.843 ft-lb/in
@Temperature -4.00 °F
ASTM D256
 0.550 J/cm
@Temperature 23.0 °C
1.03 ft-lb/in
@Temperature 73.4 °F
ASTM D256
Charpy Impact Unnotched  1.70 J/cm²
@Temperature -20.0 °C
8.09 ft-lb/in²
@Temperature -4.00 °F
DIN 53453
 1.70 J/cm²
@Temperature -40.0 °C
8.09 ft-lb/in²
@Temperature -40.0 °F
DIN 53453
 1.90 J/cm²
@Temperature 23.0 °C
9.04 ft-lb/in²
@Temperature 73.4 °F
DIN 53453
 
Electrical PropertiesMetricEnglishComments
Dielectric Strength 25.0 kV/mm
@Thickness 2.00 mm
635 kV/in
@Thickness 0.0787 in
IEC 243-1
Comparative Tracking Index >= 600 V>= 600 VIEC 112
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 163 °C325 °FASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 142 °C288 °FASTM D648
Vicat Softening Point 129 °C264 °F50°C/h 50N; ISO 306
Flammability, UL94 HB
@Thickness 1.50 mm
HB
@Thickness 0.0591 in
Oxygen Index 20 %20 %ISO 4589
 
Processing PropertiesMetricEnglishComments
Melt Temperature 220 - 250 °C428 - 482 °F
Mold Temperature 50.0 - 70.0 °C122 - 158 °F
 
Descriptive Properties
Heat Resistance - Ball Test (125°C)YIEC 335
Heat Resistance - Ball Test (165°C)NIEC 335
Injection Speedhigh
Needle Burner TestN1.47 mm
 N3.05 mm

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PLATI100 / 50098

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.