MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Mateck Sodium Chloride (NaCl)
Categories: Ceramic; Halide

Material Notes: Optical crystals

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 2.17 g/cc0.0784 lb/in³
a Lattice Constant 5.64 Å5.64 Å
c Lattice Constant 5.64 Å5.64 Å
Molecular Weight 58.45 g/mol58.45 g/mol
 
Mechanical PropertiesMetricEnglishComments
Vickers Microhardness 200200MPa
Hardness, Mohs 3.03.0
Modulus of Elasticity 32.7 GPa4740 ksiin <111> direction
 43.7 GPa6340 ksiin <100> direction
Poissons Ratio 0.2030.203
Shear Modulus 12.8 GPa1860 ksiin <111> direction
 15.9 GPa2310 ksiin <100> direction
 
Thermal PropertiesMetricEnglishComments
CTE, linear 36.4 - 40.8 µm/m-°C
@Temperature -60.0 - 60.0 °C
20.2 - 22.7 µin/in-°F
@Temperature -76.0 - 140 °F
Specific Heat Capacity 0.871 J/g-°C0.208 BTU/lb-°F
Thermal Conductivity 6.15 W/m-K
@Temperature 35.0 °C
42.7 BTU-in/hr-ft²-°F
@Temperature 95.0 °F
Melting Point 801 °C1470 °F
 
Optical PropertiesMetricEnglishComments
Refractive Index 1.49061.4906n10.6
 1.3822
@Wavelength 20000 nm
1.3822
@Wavelength 20000 nm
 1.4947
@Wavelength 10000 nm
1.4947
@Wavelength 10000 nm
 1.5153
@Wavelength 6000 nm
1.5153
@Wavelength 6000 nm
 1.532
@Wavelength 1000 nm
1.532
@Wavelength 1000 nm
 1.5467
@Wavelength 546.1 nm
1.5467
@Wavelength 546.1 nm
at ne
 1.7899
@Wavelength 200 nm
1.7899
@Wavelength 200 nm
Transmission, Visible 97 %
@Wavelength 500 nm
97 %
@Wavelength 500 nm
Internal Transmittance
IR Transmittance  5.0 %
@Wavelength 20000 nm
5.0 %
@Wavelength 20000 nm
Internal Transmittance
 87 %
@Wavelength 15000 nm
87 %
@Wavelength 15000 nm
Internal Transmittance
UV Transmittance 16 %
@Wavelength 200 nm
16 %
@Wavelength 200 nm
Internal Transmittance
 
Descriptive Properties
Cleavability(100)perfect
Constants of Elastic Compliance (Pa^-1)2.285E-11S11
 -4.69E-12S12
 7.834E-11S44
Symmetrycubic
Symmetry Classm3m
Thermal Coefficient of Refractive Index-3.31E-5 to -3.73E-5at 3.39 microns for ± 60°C
Transmission Range (microns)0.2 - 20

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Sodium Chloride, NaCl (Halite)
Potters Industries Fine Grade Oil Drilling Beads
Niagara LaSalle CPO® Cold Finished Steel Bar
Potters Industries Coarse Grade Oil Drilling Beads
Guadua Bamboo

CMAT053 / 87737

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.