MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

DSM Arnite® TV4 660 PBT/PC  (discontinued **)
Categories: Polymer; Thermoplastic; Polycarbonate (PC); Polycarbonate/Polybutylene Terephthalate (PBT) Blend, Glass Filled; Polyester, TP; Polybutylene Terephthalate (PBT)

Material Notes: 30% Glass Fiber Reinforced, Low Warpage

Processing Notes (See more info below): Screw Speed: Medium. Injection Speed: Slow-Medium.

Information provided by DSM Engineering Plastics.

Artnite is a former DSM Engineering Plastics product line now with Envalior, although this specific product was discontinued prior to that transaction

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.45 g/cc0.0524 lb/in³ISO 1183
Moisture Absorption at Equilibrium 0.15 %0.15 %ISO 62; at 50% RH
Linear Mold Shrinkage  0.0030 - 0.0060 cm/cm
@Thickness 2.00 mm
0.0030 - 0.0060 in/in
@Thickness 0.0787 in
ISO 2577
 0.0050 - 0.0090 cm/cm
@Thickness 4.00 mm
0.0050 - 0.0090 in/in
@Thickness 0.157 in
ISO 2577
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Ultimate 130 MPa18900 psiISO 527
Elongation at Break 2.2 %2.2 %ISO 527
Modulus of Elasticity 9.70 GPa1410 ksiISO 527
Flexural Strength 185 MPa26800 psiISO 178
Flexural Modulus 9.70 GPa1410 ksiISO 178
Izod Impact, Notched (ISO) 10.0 kJ/m²4.76 ft-lb/in²ISO 180/1A
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 175 °C347 °FISO 75
 
Processing PropertiesMetricEnglishComments
Rear Barrel Temperature 232 - 243 °C450 - 469 °F
Middle Barrel Temperature 249 - 260 °C480 - 500 °F
Front Barrel Temperature 243 - 254 °C469 - 489 °F
Nozzle Temperature 254 - 266 °C489 - 511 °F
Melt Temperature 243 - 271 °C469 - 520 °F
Mold Temperature 38.0 - 121 °C100 - 250 °F
Drying Temperature 121 °C250 °Fto 0.02% for molding
Dry Time 2 - 4 hour2 - 4 hourdesiccant hopper dryer preferred

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PDSM174 / 30851

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.