MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

DuPont Teijin Films Mylar® M30 Polyester Film, 50 Gauge (14 µm), PVDC Coated  (discontinued **)
Categories: Polymer; Film; Thermoplastic; Polyester, TP; Polyvinyl Dichloride (PVDC); Polyvinyl Dichloride (PVDC) Coated Polyester Film

Material Notes: Data provided by DuPont Packaging Polymers.

A transparent polyester packaging film, solvent coated on both sides with a PVDC copolymer. The coating is heat sealable, and is an excellent moisture and oxygen barrier. Available in 50, 75, and 100 gauges. Used both in unsupported form, or as a component of a lamination, and can be run on both form-fill-seal and overwrap equipment. It is particularly well suited for the packaging of long shelf life or moisture-and oxygen-sensitive products.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.40 g/cc0.0506 lb/in³Average value for Mylar® films.
Moisture Vapor Transmission 0.110 cc-mm/m²-24hr-atm0.279 cc-mil/100 in²-24hr-atmASTM E96 Procedure E
Water Vapor Transmission 8.00 g/m²/day0.515 g/100 in²/dayASTM E96 Procedure E
Oxygen Transmission 0.100 cc-mm/m²-24hr-atm0.254 cc-mil/100 in²-24hr-atmor 8 cc/m²-24hr-atm for the film. ASTM D3985
Thickness 14.0 microns0.551 mil
 
Mechanical PropertiesMetricEnglishComments
Film Elongation at Break, MD 110 %110 %ASTM D882
Film Elongation at Break, TD 70 %70 %ASTM D882
Modulus of Elasticity 3.45 GPa500 ksi(stiffness), ASTM D882
Tear Strength Test 300300Graves, g; ASTM D1004
Seal Strength 201 g/25 mm201 g/in
Film Tensile Strength at Break, MD 186 MPa27000 psiASTM D882
Film Tensile Strength at Break, TD 228 MPa33100 psiASTM D882
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 121 °C250 °FNot cleared by FDA for food temperatures above this temperature.
Shrinkage 1.5 %
@Temperature 150 °C,
Time 1800 sec
1.5 %
@Temperature 302 °F,
Time 0.500 hour
Film shrinkage in oven.
 
Optical PropertiesMetricEnglishComments
Haze 7.0 %7.0 %ASTM D1003
Gloss 140 %140 %20°; ASTM D2457
Transmission, Visible 90 %90 %transparent; thickness not quantified

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Syensqo (Solvay Specialty Polymers) Diofan® P530 Polyvinylidene Chloride (PVDC)
SK Chemicals Saran® 506 Polymer
SK Chemicals Saran® 313 PVDC
SK Chemicals Saran® 2032
SK Chemicals Saran® 168

PDU659 / 33108

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.