MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

American Largetooth Aspen (Bigtooth Aspen) Wood
Categories: Wood and Natural Products; Wood; Hardwood

Material Notes: Diffuse-Porous Hardwood

Property values marked by an asterisk (*) have been taken from an unusually old reference source.

Key Words: Populus grandidentata; Lumber, Timber
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesMetricEnglishComments
Hardness, Wood Indentation 1600 N360 lb (f)Side. Force required to imbed a 0.444 inch steel ball to one-half its diameter
 2000 N450 lb (f)End. Force required to imbed a 0.444 inch steel ball to one-half its diameter
Tensile Strength, Ultimate 2.69 MPa390 psiPerpendicular to Grain*
Modulus of Rupture 0.0400 GPa5.80 ksiStatic Bending*
Flexural Yield Strength 22.1 MPa3200 psiFiber Stress at Elastic Limit; Static Bending*
Flexural Modulus 8.14 GPa1180 ksiStatic Bending*
Compressive Strength 1.86 MPa270 psiPerpendicular to Grain*
 14.7 MPa2130 psiParallel to Grain*
 18.8 MPa2720 psiMax Crushing Strength Parallel to Grain*
Shear Strength 5.58 MPa810 psiParallel to Grain*
Impact 2.72.7in-lb/in³; Work to Elastic Limit; Unseasoned Sample; Impact Bending*
 76007600psi; Fiber Stress at Elastic Limit; Unseasoned Sample; Impact Bending*
Work to Elastic Limit 0.00345 J/cm³0.500 in-lb/in³Static Bending*
Work to Maximum Load 0.0421 J/cm³6.10 in-lb/in³Static Bending*
 
Thermal PropertiesMetricEnglishComments
Thermal Conductivity 0.0980 W/m-K0.680 BTU-in/hr-ft²-°FOven Dry
 0.118 W/m-K0.820 BTU-in/hr-ft²-°F12% Moisture Content

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
North American Quaking Aspen (Trembling Aspen) Wood
American Balsam Fir Wood
American Maple, Rock (Sugar Maple)
American Eastern White Pine Wood
American Ponderosa Pine Wood

PTSA030 / 71241

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.