MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

CRP  Windform

Braskem GR900PP-CF Carbon Fiber Reinforced Polypropylene 3D Printing Pellets
Categories: Polymer; 3D Printing/Additive Manufacturing Polymer; Thermoplastic; Polypropylene (PP); Polypropylene, Carbon Fiber Filled

Material Notes: GR900PP-CF is an engineering-grade composite made from 100% recycled carbon fiber (CF) and is designed to provide robust mechanical performance while maintaining a high degree of printability for complex structures. GR900PP-CF provides engineering level performance without compromising any of PP’s inherent properties which include light weight, water resistance (no drying needed), chemical resistance, and impact resistance.

Reported property values are from printed parts; tensile specimens were oriented parallel to the layer direction.

Information provided by Braskem.

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 0.910 g/cc0.0329 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 6363ASTM D2240
Tensile Strength 41.0 MPa5950 psiASTM D638
Elongation at Break 1.3 %1.3 %ASTM D638
Modulus of Elasticity 6.38 GPa925 ksiASTM D638
Flexural Modulus 4.512 GPa654.4 ksiChord Modulus; ASTM D790
Charpy Impact, Notched 1.16 J/cm²5.52 ft-lb/in²ISO 179
Impact Test  2.30 J
@Thickness 3.00 mm,
Temperature 23.0 °C
1.70 ft-lb
@Thickness 0.118 in,
Temperature 73.4 °F
Drop Impact Peak Energy; 2.73m/s; ASTM D3763
 3.50 J
@Thickness 3.00 mm,
Temperature 0.000 °C
2.58 ft-lb
@Thickness 0.118 in,
Temperature 32.0 °F
Drop Impact Peak Energy; 2.73m/s; ASTM D3763
 5.20 J
@Thickness 3.00 mm,
Temperature -20.0 °C
3.84 ft-lb
@Thickness 0.118 in,
Temperature -4.00 °F
Drop Impact Peak Energy; 2.73m/s; ASTM D3763
Puncture Energy  5.20 J
@Thickness 3.00 mm,
Temperature 23.0 °C
3.84 ft-lb
@Thickness 0.118 in,
Temperature 73.4 °F
Drop Impact Puncture Energy; 2.73m/s; ASTM D3763
 5.40 J
@Thickness 3.00 mm,
Temperature -20.0 °C
3.98 ft-lb
@Thickness 0.118 in,
Temperature -4.00 °F
Drop Impact Puncture Energy; 2.73m/s; ASTM D3763
 6.20 J
@Thickness 3.00 mm,
Temperature 0.000 °C
4.57 ft-lb
@Thickness 0.118 in,
Temperature 32.0 °F
Drop Impact Puncture Energy; 2.73m/s; ASTM D3763
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 158 °C316 °FASTM D648
Vicat Softening Point 150 °C302 °F10 N; ASTM D1525

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PBRAS692 / 291045

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.