MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Mateck Calcium Fluoride (CaF2)
Categories: Ceramic; Halide

Material Notes: Optical crystals

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 3.18 g/cc
@Temperature 20.0 °C
0.115 lb/in³
@Temperature 68.0 °F
Solubility 0.0016 ppm0.0016 ppm
a Lattice Constant 5.462 Å5.462 Å
Molecular Weight 78.08 g/mol78.08 g/mol
 
Mechanical PropertiesMetricEnglishComments
Vickers Microhardness 16501650MPa
Hardness, Mohs 4.04.0
Modulus of Elasticity 89.9 GPa13000 ksi<111> direction
 146.1 GPa21190 ksi<100> direction
Poissons Ratio 0.2160.216
Shear Modulus 33.8 GPa4900 ksi<111> direction
 47.6 GPa6900 ksi<100> direction
 
Thermal PropertiesMetricEnglishComments
CTE, linear 16.5 - 19.4 µm/m-°C
@Temperature -60.0 - 60.0 °C
9.17 - 10.8 µin/in-°F
@Temperature -76.0 - 140 °F
Specific Heat Capacity 0.8876 J/g-°C0.2121 BTU/lb-°F
Thermal Conductivity 9.71 W/m-K
@Temperature 36.0 °C
67.4 BTU-in/hr-ft²-°F
@Temperature 96.8 °F
Melting Point 1418 °C2584 °F
 
Optical PropertiesMetricEnglishComments
Refractive Index 1.29961.2996n10.6
 1.43491.4349n3
 1.2299
@Wavelength 12000 nm
1.2299
@Wavelength 12000 nm
 1.3856
@Wavelength 6000 nm
1.3856
@Wavelength 6000 nm
 1.4239
@Wavelength 2000 nm
1.4239
@Wavelength 2000 nm
 1.4951
@Wavelength 200 nm
1.4951
@Wavelength 200 nm
Transmission, Visible 97 %
@Wavelength 500 nm
97 %
@Wavelength 500 nm
Internal Transmittance
IR Transmittance  19 %
@Wavelength 10000 nm
19 %
@Wavelength 10000 nm
Internal Transmittance
 97 %
@Wavelength 7000 nm
97 %
@Wavelength 7000 nm
Internal Transmittance
UV Transmittance 87 %
@Wavelength 200 nm
87 %
@Wavelength 200 nm
Internal Transmittance
 
Descriptive Properties
Cleavability(111)perfect
Constants of Elastic Compliance (Pa^-1)-1.53E-12S12
 2.958E-11S44
 6.83E-12S11
Symmetrycubic
Symmetry Classm3m
Thermal Coefficient of Refractive Index-0.95E-5 to -1.17E-5
Thermal Stability, °C20±2
Transmission Range (microns)0.15 - 9

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Calcium Fluoride, CaF2 (Fluorite)
MarkeTech Lutetium Aluminum Garnet:Cerium (LAG:Ce) Scintillator Crystal
Reade Advanced Materials Garnet Powder (Fe3Al2(SiO4)3)
Harris Acoustic Sensors ELL-1203 Aluminum Substituted Narrow Line Width Garnet (3-Series)
Aluminum 5052-H32

CMAT041 / 87725

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.